Results 1 to 10 of 10

Thread: Can I use propane or LPG gas for welding?

  1. #1
    Join Date
    Jul 2020
    Location
    Dubai
    Posts
    19
    Post Thanks / Like

    Can I use propane or LPG gas for welding?

    Can I use propane or LPG gas for welding?

  2. #2
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    1,337
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Murphy's Golden Rule: Whoever has the gold, makes the rules.

  3. Likes shovelon liked this post
  4. #3
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,819
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Short answer and long answer are both no...

    I like it for heating and cutting though.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #4
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    243
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Quote Originally Posted by shasti View Post
    Can I use propane or LPG gas for welding?
    Depending on what you are doing,, possibly brazing or silver soldering would work?
    With brazing, you could use propane,, especially if you buy a "TurboTorch".

    I have several sizes of TurboTorch tips, even the biggest T-6 tip, that torch is amazing.
    I believe I could braze 3/4 inch solid steel bar to 1/4X2 inch steel bar.

    Car body repairs should be easy,, and no acetylene is needed.

    If your parts are smaller, a smaller (lower cost) tip is adequate.

  6. #5
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,209
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    You absolutely can, just not in the manor these guys are thinking of.

    You just need one of these little honeys and you can weld with propane all day long!
    Attached Images Attached Images  

  7. Likes 12V71, Dave66, farmersammm, Louie1961 liked this post
  8. #6
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,624
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    I agree with MinnesotaDave.
    It possible to but will not give good job.
    I did try propane and oxygen one time when about 14 it was not good.

    Dave

    Quote Originally Posted by shasti View Post
    Can I use propane or LPG gas for welding?

  9. #7
    Join Date
    Oct 2014
    Posts
    3,551
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Need a neutral flame for gas welding which is only possible with acetylene. What do think all extra oxygen from burning propane is going to do?

  10. #8
    Join Date
    Jul 2020
    Location
    Dubai
    Posts
    19
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Thank you for your advice.

  11. #9
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    243
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    Quote Originally Posted by Welder Dave View Post
    Need a neutral flame for gas welding which is only possible with acetylene. What do think all extra oxygen from burning propane is going to do?
    I thought a neutral flame was possible with any fuel, even charcoal,,
    IMHO, neutral indicates neither excess oxygen, or inadequate oxygen.

    If the flame is neutral, the flame is at its highest BTU output, and probably the highest measurable temperature.


  12. #10
    Join Date
    Oct 2014
    Posts
    3,551
    Post Thanks / Like

    Re: Can I use propane or LPG gas for welding?

    No. Actetylene is hottest with an oxidizing flame, 6300*F neutral is around 5850*F carburizing around 5700*F depending on how much O2 is added. Sometimes you see terms like 2X feather or 3X feather. That refers to the outer feather of the flame and is adjusted by the amount of O2. Only oxy/acet. can produce a neutral flame with enough heat to melt steel. Oxy/propane (or other fuel) can have a flame hot enough to melt steel but it is an oxidizing flame so won't produce a sound weld. For brazing where you don't melt the steel propane and other fuel gases can be used.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,163,628.38925 seconds with 14 queries