    Engine Driven Welder Electrical Issue

    Hey all.
    I have a Hobart Champion 10000, pretty much a bare bones Bobcat 225. 20 horse Kohler engine. A couple months ago I mistakenly left the ignition switch in the "run" position for a couple weeks. The welder had an electric fuel pump on it, and one day while I was working in my garage, I heard the pump make the noise it makes when it's typically turned on. This is when I discovered I left the ignition on.

    I assumed I burned the pump out so I installed a mechanical one I had laying around. No luck. So after a lot of investigating, I discovered the fuel shutoff solenoid is not getting power in the "run" position. It does get power in the "start" position while cranking, so the welder will fire up for about 1 sec and then die.

    I have checked the wires for shorts or breaks, the low oil pressure switch is working correctly, the PC board doesn't have any crap stains on it and the "run" wire doesn't pass through the board anyway, the ignition switch is testing fine, the fuse coming from the starter isn't blown. Really not sure what else to check. Does anyone have a suggestion?

    The serial number is LC471626. I believe it's an 04 model.

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,392
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    I'd double check the OP switch. It has to close to feed 12V+ from RUN to the fuel shut-off solenoid, the ignition relay CR1 and to wire #20 of PC1 PLG5 pin 5. START does the same thing thru diode D8 which is why it'll run in START.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. Likes mla2ofus, Shwoody liked this post
  4. #3
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,392
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    You can bypass the OP switch with a jumper and see if it runs in RUN.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  5. Likes mla2ofus liked this post
  6. #4
    Join Date
    Mar 2019
    Location
    Colorado Springs, CO
    Posts
    30
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    Interesting development:
    Last night I made a little bypass jumper which did not solve the problem, and bench tested the oil pressure sensor, which tested fine. Figured I'd go try the jumper one last time before responding though. The welder fired right up. Then I tried it without bypassing the oil pressure sensor and it also started fine.

    The battery was reading 12.5v yesterday and it was cranking strong but I hooked up the trickle charger overnight anyway. Before charging, the fuel solenoid was seeing 10.5v (an online article said that was within acceptable range) in the start position and nothing in the run position. Now it's reading over 12v in the run position.
    Maybe I win the dingus award of the day but wouldn't I have been getting SOME voltage at the fuel solenoid, even if the battery was slightly low?

  7. #5
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,298
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    I just replaced the ignition switch wire terminals on mine for a similar issue. They just weren’t making good contact. With the new terminals on there is a lot more tension in the plug when installing it.

  8. #6
    Join Date
    Oct 2014
    Posts
    1,186
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    Quote Originally Posted by Shwoody View Post
    Interesting development:
    Last night I made a little bypass jumper which did not solve the problem, and bench tested the oil pressure sensor, which tested fine. Figured I'd go try the jumper one last time before responding though. The welder fired right up. Then I tried it without bypassing the oil pressure sensor and it also started fine.

    The battery was reading 12.5v yesterday and it was cranking strong but I hooked up the trickle charger overnight anyway. Before charging, the fuel solenoid was seeing 10.5v (an online article said that was within acceptable range) in the start position and nothing in the run position. Now it's reading over 12v in the run position.
    Maybe I win the dingus award of the day but wouldn't I have been getting SOME voltage at the fuel solenoid, even if the battery was slightly low?
    Is there a relay in the circuit to the fuel solenoid ? maybe it wasn't getting enough voltage to switch relay on if there is any such relay at all. ???

  9. #7
    Join Date
    Mar 2019
    Location
    Colorado Springs, CO
    Posts
    30
    Post Thanks / Like

    Re: Engine Driven Welder Electrical Issue

    I didn't see any sort of relay. All the terminals felt secure but maybe it was just a poor connection somewhere that is now making contact after being messed with. Hopefully the problem doesn't come back but if it does, I'll cross that bridge when I come to it ha.

    Thank you everyone for the advice.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,081,163.08298 seconds with 14 queries