Results 1 to 21 of 21

Thread: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

  1. #1
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    This is my latest work, a fully handmade tank model, used minimum tools in my primitive workshop, Let me know your ideas guys!

    Name:  craft channel out2.00_00_09_09.Still003.jpg
Views: 468
Size:  61.1 KBName:  craft channel out2.00_00_55_33.Still012.jpg
Views: 468
Size:  43.9 KBName:  craft channel out2.00_00_53_28.Still010.jpg
Views: 486
Size:  73.9 KBName:  craft channel out2.00_00_40_06.Still008.jpg
Views: 467
Size:  68.6 KBName:  craft channel out2.00_00_25_23.Still006.jpg
Views: 462
Size:  42.3 KB


  2. #2
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    1,952
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Awesome!!
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 120

    10FtDrillBit.com

  3. Likes scoobyz, 12V71 liked this post
  4. #3
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by wb4rt View Post
    Awesome!!
    Thank you!

  5. #4
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,899
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    That is amazing work, my compliments........Mike

  6. Likes scoobyz liked this post
  7. #5
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Thanks Mike

  8. #6
    Join Date
    Dec 2011
    Location
    Tampa FL
    Posts
    1,229
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    That is amazing, the attention to detail and craftsmanship. Do you know how many hours to build?
    Mike

  9. Likes scoobyz liked this post
  10. #7
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by scoobyz View Post
    Thanks Mike
    It takes 2-3 weeks with my other works

  11. #8
    Join Date
    Dec 2018
    Posts
    5,618
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    That is absolutely NICE!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!

  12. Likes scoobyz liked this post
  13. #9
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by farmersammm View Post
    That is absolutely NICE!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!
    Thank you!

  14. #10
    Join Date
    Oct 2018
    Posts
    14
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Just beautiful work. Incredible patience and skill with simple tools. Nice video, also!
    Dave
    WelditU.com

    Lincoln Weld-Pak 140HD
    Hobart Handler 140

  15. Likes scoobyz liked this post
  16. #11
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,377
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    I’ve always had a certain fascination with hand-crafted models
    of ships, planes and trains. That’s the first tank model I’ve seen
    (other than plastic kits). Beautiful work. Good video too.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  17. Likes scoobyz liked this post
  18. #12
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,241
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    As shown, it not the tools in the hand, but the hands the tools are in. Thanks for posting the images and the video it show you love what you do.
    DIY CNC Plasma table USB BOB Price THC
    Hypertherm 65
    Everlast PowerTig 255 EXT
    Miler 180 Mig
    13" metal lathe
    Mill/ Drill
    ECT, ECT,

  19. Likes MinnesotaDave, 12V71, scoobyz liked this post
  20. #13
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,864
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Very impressive!! Looks awesome
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  21. Likes scoobyz liked this post
  22. #14
    Join Date
    Feb 2016
    Location
    Oregon
    Posts
    110
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    VERY impressive work. You demonstrate great skill.

  23. Likes scoobyz liked this post
  24. #15
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by WelditU View Post
    Just beautiful work. Incredible patience and skill with simple tools. Nice video, also!
    Thank you so much!

  25. #16
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by jpump5 View Post
    I’ve always had a certain fascination with hand-crafted models
    of ships, planes and trains. That’s the first tank model I’ve seen
    (other than plastic kits). Beautiful work. Good video too.
    Thank you so much, more works on the way!

  26. #17
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by acourtjester View Post
    As shown, it not the tools in the hand, but the hands the tools are in. Thanks for posting the images and the video it show you love what you do.
    Thank You sir!

  27. #18
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by MinnesotaDave View Post
    Very impressive!! Looks awesome
    Thank You!!!

  28. #19
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,899
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    .....more works on the way!
    I certainly hope so, you can't show one work of art and leave it at that :-)...............Mike

  29. Likes scoobyz liked this post
  30. #20
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    963
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    What everybody above has said with another Awesome.

  31. Likes scoobyz liked this post
  32. #21
    Join Date
    Jul 2021
    Location
    Sri lanka
    Posts
    11
    Post Thanks / Like

    Re: I turned a Brass Sheet Into a Golden T-55 (Soviet Main Battle Tank)

    Quote Originally Posted by lars66 View Post
    What everybody above has said with another Awesome.
    Thank You!

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,285,245.23960 seconds with 13 queries