    Power iMIG 230i 120v

    I have iMIG 230i and currently only have 3300/3650 watt, 120v 30 amp >3% clean power generator, will be getting 11000 watt 240v >5% generator.

    But for now can the 230i run on 120v 30 amp?
    If so how thick of steel can it weld on 120v?

    If I understand it correctly the 230i will run on 120v, but wanted to be sure the 3300/3650 watt 120v 30 amp generator is ok to use for now, don’t want to damage my new machine!
    :-)

    Cheers, Allen

  2. #2
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    It'll need every bit of 3600 watts.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  3. #3
    Join Date
    Nov 2014
    Posts
    47
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    If it’s not a good idea to use this small of a generator, I’ll not take a chance of damaging my iMIG 230.
    If it will work and not harm the welder, can it weld ⅛”?

    Cheers, Allen

  4. #4
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    If your generator is ok and in good shape, it won't be a problem as long as you don't max it out. It should weld 1/8". If your generator starts to load up significantly, stop though. Simple as that, as long as it is clean power rated. Is this an inverter type? (Also don't use it on ECO idle).
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  5. #5
    Join Date
    Nov 2014
    Posts
    47
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    It is almost new Firman inverter generator, has switch to turn off eco weld.

    I’m going to get a Westinghouse WPro 8500/11000 watt >5% THD clean power 240v 35 amp running and 48 amp surge when they are available. They have been out of stock for while.

    Cheers, Allen

  6. #6
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    less than, not greater than 5%. You posted greater than.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  7. #7
    Join Date
    Nov 2014
    Posts
    47
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    Oops lol yes, was supposed to be less than. Lol

  8. #8
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    Quote Originally Posted by abosely View Post
    It is almost new Firman inverter generator, has switch to turn off eco weld.

    I’m going to get a Westinghouse WPro 8500/11000 watt >5% THD clean power 240v 35 amp running and 48 amp surge when they are available. They have been out of stock for while.

    Cheers, Allen
    Nothern Tool has one that is similar. Not sure if they have it in stock.

    https://www.northerntool.com/shop/to...3128_200913128
    1st on WeldingWeb to have a scrolling sig!



  9. #9
    Join Date
    Sep 2012
    Location
    Cupertino, California
    Posts
    364
    Post Thanks / Like

    Re: Power iMIG 230i 120v

    Just keep that welder's power to running in 120 volts for now. And don't go greater than 110 amps max, when plugged into your generator's 30-amp 120v outlet. So, yes, you are good for roughly 1/8"-thick steel (~11-gauge). And I second on what Lugwelder states about switching off the ECO-mode. My .02 cents. I like lots of safety margin, whenever I use a generator to run a welder. (My lightweight/portable welder, for small jobs, is a Harbor Freight Titanium 125 Amp fluxcore welder, which I sometimes use at a maximum 115 amps when hooked into a 3800-watt WEN generator's 120v, 30-amp outlet. It works flawlessly.)
    Last edited by Agape Guy; 08-24-2021 at 07:20 PM.
    Agape Guy
    Everlast Power I-MIG 200 (dual voltage)
    Everlast SM200N Spool Gun (aluminum mig welding)
    Everlast PowerArc 200 stick
    Harbor Freight Titanium 125 Easy Flux
    Hypertherm Powermax 30 plasma cutter
    Way too many power tools

  10. Likes lugweld liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,263,187.37828 seconds with 19 queries