Miller Bobcat 225 NT won't stay running
I have a Bobcat 225 NT with an Onan P216 that will start and run, but dies as soon as I let off the ignition. New ignition switch. Neighbor came over and ran a hot wire from battery + to coil +. It started up, and ran until he removed wire - didn't run it very long. He know's enough about small engines to try that, and I know even less than that. I'd really appreciate any help that anyone can offer! --------------------- John
John
Miller 320 A/BP
Miller Auto Arc 50
Miller 150 STH
Miller 225NT Generator
Lincoln SP-200
PlasmaFix 50S Plasma Welder
"Cheap Azz" Plasma Cutter
Machine Shop
-
-
Re: Miller Bobcat 225 NT won't stay running
Originally Posted by
jptech
I have a Bobcat 225 NT with an Onan P216 that will start and run, but dies as soon as I let off the ignition. New ignition switch. Neighbor came over and ran a hot wire from battery + to coil +. It started up, and ran until he removed wire - didn't run it very long. He know's enough about small engines to try that, and I know even less than that. I'd really appreciate any help that anyone can offer! --------------------- John
Oil pressure switch. Or you have no oil pressure.
-
Re: Miller Bobcat 225 NT won't stay running
Thank You!! I bypassed the switch, it started right up and ran. ---------------------- John
John
Miller 320 A/BP
Miller Auto Arc 50
Miller 150 STH
Miller 225NT Generator
Lincoln SP-200
PlasmaFix 50S Plasma Welder
"Cheap Azz" Plasma Cutter
Machine Shop
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Miller Bobcat 225 NT won't stay running
Originally Posted by
jptech
Thank You!! I bypassed the switch, it started right up and ran. ---------------------- John
Had that problem 3 times on the Onans, first and third time was the switch, second time nobody checked the oil level.
-
Post Thanks / Like - 1 Likes, 0 Dislikes