    Settle this debate on a weld symbol....

    So going through our company's standard operating procedure test that is give to new applicates. A question/debate arose about a ground flush weld symbol. Look at the picture. If you saw the picture on the left and were asked "What the darkened line under the weld symbol indicates, what would you answer?
    Name:  GROUND FLUSH QUESTION.jpg
Views: 442
Size:  55.0 KB

  2. #2
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    1,899
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    I would say the first one is flush weld on top, just left as welded no excess reinforcement.
    On the second symbol, if you want it ground flush on the bottom side you should have the 'G" beneath the line so the weld would be ground flush on the bottom since the arrow is pointing to the bottom of the weld and the symbol is on the bottom which is the arrow side of the line.
    Mind you it's been years so I could be full of it too LOL ............Mike

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,808
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    I would contact the draftsman/engineer how made drawing and clear instructions.
    They come some thing off wall sometimes.
    It save money too.
    FYI They come new symbol every year and old symbol is just same thing.
    When I first started it was a wall chart with all symbols and very clear, today it takes book and not so clear.

    Dave

    Quote Originally Posted by MrsVPH83 View Post
    So going through our company's standard operating procedure test that is give to new applicates. A question/debate arose about a ground flush weld symbol. Look at the picture. If you saw the picture on the left and were asked "What the darkened line under the weld symbol indicates, what would you answer?
    Name:  GROUND FLUSH QUESTION.jpg
Views: 442
Size:  55.0 KB
    Last edited by smithdoor; 07-24-2021 at 08:27 PM.

  4. #4
    Join Date
    Mar 2012
    Location
    Australia
    Posts
    729
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    Quote Originally Posted by MrsVPH83 View Post
    So going through our company's standard operating procedure test that is give to new applicates. A question/debate arose about a ground flush weld symbol. Look at the picture. If you saw the picture on the left and were asked "What the darkened line under the weld symbol indicates, what would you answer?
    Name:  GROUND FLUSH QUESTION.jpg
Views: 442
Size:  55.0 KB
    the first one with the solid line under the square butt symbol I think is a mistake or for some sort of specialised welding process (flash but, friction stir, plasma welding etc all have process specific symbols that I'm not familiar with).

    the second one is a square butt weld ground flush on the same side as the arrow.

  5. #5
    Join Date
    Oct 2014
    Posts
    3,763
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    Normally it would say grind or maybe they use a G now. Arrow side is always on the bottom of the reference line if I remember correctly. Sometimes there is a tail on the reference line that can show more info. In the first one I think it means flush but with no other info. don't know if the weld should just be flush or it should flush by using another means like grinding or machining. It has been a long time for me too since I've had to reference blueprints with welding symbols.

  6. #6
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,872
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    The line either way is a profile symbol in the as welded condition. If someone mechanically flushes out the weld they are in violation of the intent. Looks like a tig weld application to me to keep the square bevel joint flush. I have see similar welds where the welds were ground flush without permission and were rejected.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  7. #7
    Join Date
    Sep 2013
    Location
    Holland
    Posts
    225
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    Quote Originally Posted by MrsVPH83 View Post
    So going through our company's standard operating procedure test that is give to new applicates. A question/debate arose about a ground flush weld symbol. Look at the picture. If you saw the picture on the left and were asked "What the darkened line under the weld symbol indicates, what would you answer?
    Name:  GROUND FLUSH QUESTION.jpg
Views: 442
Size:  55.0 KB
    Name:  Schermafbeelding 2021-07-31 130732.png
Views: 204
Size:  63.5 KB

  8. #8
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,808
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    I seen draftsman/engineer put symbol out book and not what want or high cost to do the job.
    I found call and find out want the really want.

    Dave

    Quote Originally Posted by denlow60 View Post
    Name:  Schermafbeelding 2021-07-31 130732.png
Views: 204
Size:  63.5 KB

  9. #9
    Join Date
    Nov 2006
    Posts
    14
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    It is simply a square groove weld with a flush contour. It does not specify how to achieve that. If there were a G below it, it would be ground flush. If there were an M below it, it would indicate machined flushl. Being nothing below it, it may simply mean weld it as close to flush as possible or no excessive crown. It would be best to ask the person that drew it.

  10. #10
    Join Date
    Oct 2014
    Posts
    3,763
    Post Thanks / Like

    Re: Settle this debate on a weld symbol....

    I think the debate is that you shouldn't have to ask for clarification, it should be very clear on the blueprint. What if the blueprints came from another country or something, are you going to wait for who knows how long to get that clarification.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,253,881.26732 seconds with 12 queries