    Welding Procedure/Weld Type for Heavy W Trusses

    Hello,
    I am new here and I am looking for help/recommendation on welding procedure that my client has asked me to provide. I do steel detailing and engineering and we are working on the project where 3 heavy trusses were designed. Top and bottom chords are W14x311 and diagonals are made of W12x152 and W14x120. Each truss is onlcy 6'-6" deep therefore directly welded connections were chosen and designed. Flanges in all diagonal get CJP to top and bottm chord's flange and web is welded with fillet weld. The diagonal angle varies from 30 degrees to 55 degrees. I discussed with my client (Steel contractor) that they will bevel the flange on one side with 1/4" root opening, 1"x1/4" backing bar and full penetration weld. Is there a pre-qualified procedure in AWS D1.1 for this type of joint? I know there is a TC-U4a-GF a single bevel-groove weld for T-joint but in my case diagonals to chord connections are not at 90 degrees..Any help will be much appreciated. Typical connection attached.
    Thanks in advance

    Jacek
    Attached Images Attached Images  

  2. #2
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,787
    Post Thanks / Like

    Re: Welding Procedure/Weld Type for Heavy W Trusses

    Not to sound rude but as an engineer, isn't that your job to know this stuff. If you engineered the truss per load you should really know the weld procedures.

  3. Likes flushcut, Dave66 liked this post
  4. #3
    Join Date
    Jul 2008
    Posts
    3,048
    Post Thanks / Like

    Re: Welding Procedure/Weld Type for Heavy W Trusses


  5. Likes Dave66 liked this post
  6. #4
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,800
    Post Thanks / Like

    Re: Welding Procedure/Weld Type for Heavy W Trusses

    I like that work it like good old days.
    I found check with engineer is always good thing.

    Dave

    Quote Originally Posted by Jacek_JJSA View Post
    Hello,
    I am new here and I am looking for help/recommendation on welding procedure that my client has asked me to provide. I do steel detailing and engineering and we are working on the project where 3 heavy trusses were designed. Top and bottom chords are W14x311 and diagonals are made of W12x152 and W14x120. Each truss is onlcy 6'-6" deep therefore directly welded connections were chosen and designed. Flanges in all diagonal get CJP to top and bottm chord's flange and web is welded with fillet weld. The diagonal angle varies from 30 degrees to 55 degrees. I discussed with my client (Steel contractor) that they will bevel the flange on one side with 1/4" root opening, 1"x1/4" backing bar and full penetration weld. Is there a pre-qualified procedure in AWS D1.1 for this type of joint? I know there is a TC-U4a-GF a single bevel-groove weld for T-joint but in my case diagonals to chord connections are not at 90 degrees..Any help will be much appreciated. Typical connection attached.
    Thanks in advance

    Jacek
    HF 170 welder
    HF 4x6 band saw
    South Bend 9N
    Mill
    B&D mag drill
    Victor torch

  7. #5
    Join Date
    Nov 2006
    Posts
    14
    Post Thanks / Like

    Re: Welding Procedure/Weld Type for Heavy W Trusses

    Because of the angles involved you will need to specify this procedure. Take a look at section 2 and research "z-loss" this will need to be taken into consideration with this detail.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,631,986,774.39374 seconds with 15 queries