    I have a Harris 25-500 regulator I have been using with CO2 to feed a proportional mixer. The regulator started creeping up from the set pressure 100 PSI, I will try a new seat in the regulator. I have been using this for several years, Harris lists several gases for the regulator but not CO2. I am using a fairly low flow of CO2 and have not seen any icing the mix ratio is 75/25 argon / CO2 at most. I attribute the problem to be simply time/wear, it worked fine for years. Is there some compelling reason this regulator should not be used in this application?
    Steve from SoCal now in Hutch

    Miller Dynasty 300DX Coolmate3 Speedway Torch
    Miller XMT 450 MPa plus with D-74 MPa Plus
    Miller Bobcat 225 NT
    Hypertherm Powermax 45
    And a whole bunch of machines

  2. #2
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,238
    Post Thanks / Like

    Re: Regulator for CO2

    Some regulators are dual purpose (C02-Argon), there are people the repair regulators.
    DIY CNC Plasma table USB BOB Price THC
    Hypertherm 65
    Everlast PowerTig 255 EXT
    Miler 180 Mig
    13" metal lathe
    Mill/ Drill
    ECT, ECT,

  3. #3
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,796
    Post Thanks / Like

    Re: Regulator for CO2

    Quote Originally Posted by acourtjester View Post
    Some regulators are dual purpose (C02-Argon), there are people the repair regulators.
    He already mentioned it wasn't rated for CO₂ though. Quick google search confirms this. But who knows why it's acting up. I would call up harris and see what they say.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,631,949,796.06754 seconds with 11 queries