    honey colored filler for stainless welding

    I'm getting ready to weld up some stainless headers and I see other tig welds that the filler looks real clean and has a honey color to it, I don't think its silicon bronze because of the puddle.
    Any help is appreciated, thanks, Oj

  2. #2
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    852
    Post Thanks / Like

    Re: honey colored filler for stainless welding

    the temperature of the weld when exposed to atmosphere, no longer covered by the shielding gas, determines the color of the stainless. When tacking, and holding the gas on a short weld will often give you a bright shiny silver spot. Lingering to long , or not moving fast enough will get you the darker blues, and purples. If you have bad gas coverage it can be dull gray to black.

    Name:  DSCF1189.jpg
Views: 198
Size:  41.2 KB

    this was 304 stainless welded using 1/16" 308L , you can see where the gas coverage ended. Sometimes you can lift your helmet, and watch the metal turn color after the post flow ends.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  3. #3
    Join Date
    Jul 2008
    Posts
    3,044
    Post Thanks / Like

    Re: honey colored filler for stainless welding

    OP, I think "straw" is the word you're looking for, and it's dependent on the temperature of your weld when it's exposed to air.


  4. #4
    Join Date
    Oct 2014
    Posts
    3,763
    Post Thanks / Like

    Re: honey colored filler for stainless welding

    Perfect heat, travel speed and an experienced welder can make beautifully colored Tig welds. If they're stray color is generally about as close to perfection as you can get. Should note penetration and bead profile are also part of it. Stray colored part in post 2 is not anywhere near perfection.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,631,947,165.76664 seconds with 14 queries