    Finally Fixed The Mig!

    So I have this Thermal Arc 211 I mig welder. When I bought it 7-8 years ago it worked fine. Over the last several years I noticed it wasn't welding up to par (I have not used it much). I come to discover that the drive wheels were slipping on the wire (changing the tension did nothing). I used a trick that I picked up off another member here. I switched out the drive wheel to the serrated wheel meant for flux core. Problem solved.......and you need very little tension on the drive wheel.

  2. Likes MinnesotaDave liked this post
  3. #2
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,802
    Post Thanks / Like

    Re: Finally Fixed The Mig!

    If you are using the knurled roller on solid steel wire, it will over time clog up the liner as it bites and chews on the wire. The indentations left on the wire may also chew up the tip as they slide in the bore, elongating it.
    1st on WeldingWeb to have a scrolling sig!



  4. #3
    Join Date
    Apr 2009
    Posts
    90
    Post Thanks / Like

    Re: Finally Fixed The Mig!

    I agree with what Oscar said, but my Challenger 172 only came with a knurled roller. While not being much of a welder, I have used it as said, with light tension on solid wire for years. It does create a little dust and you may need to blow out the liner occasionally, but this has worked for me.

  5. #4
    Join Date
    Dec 2011
    Posts
    968
    Post Thanks / Like

    Re: Finally Fixed The Mig!

    All good points guys......thank you!

  6. #5
    Join Date
    Apr 2016
    Location
    CA
    Posts
    7,902
    Post Thanks / Like

    Re: Finally Fixed The Mig!

    Replacing a liner every 3 to 5 rolls of wire is a small price to pay to have a welder that welds good when using knurled rollers. I use knurled rollers for solid wire with minimal wire tension.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,256,860.73952 seconds with 14 queries