    I thought I knew how to read these, but I guess I don't. When was this tank tested?

    Name:  date.jpg
Views: 738
Size:  71.1 KB

  2. #2
    Join Date
    Oct 2018
    Posts
    14
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    Looks like April 2021.
    Dave
    WelditU.com

    Lincoln Weld-Pak 140HD
    Hobart Handler 140

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,896
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    When go fill tank they tell the date.
    Most tanks need to be tested every 5 years.
    Some new tanks well 10 years.

    Dave

    FYI the marks after the date [+*] is 10 years test date and over fill by 10%
    https://welditmyself.com/gas-cylinder-date-stamp/#12-would-you-like-to-see-an-argon-tank-date-stamp-example

    Quote Originally Posted by Wolfman View Post
    I thought I knew how to read these, but I guess I don't. When was this tank tested?

    Name:  date.jpg
Views: 738
Size:  71.1 KB
    Last edited by smithdoor; 07-31-2021 at 06:26 PM.

  4. #4
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    1,029
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    + sign followed by a star sign means test is good for 10 years. Most customer owned cylinders only get the +. I did a fair amount of hydrotesting back in the mid 80's
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  5. #5
    Join Date
    Nov 2013
    Location
    MO
    Posts
    40
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    Quote Originally Posted by smithdoor View Post
    FYI the marks after the date [+*] is 10 years test date and over fill by 10%
    That is the part I actually understood.

    It is the 18 that had me confused.

  6. #6
    Join Date
    Nov 2013
    Location
    MO
    Posts
    40
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    Doh! IA18 is the stamp of a specific independent tester. Confusion over!

  7. #7
    Join Date
    May 2007
    Posts
    4,589
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    i got one the same, but follwed by a '14 instead of '21, and i'm 1500 mi from u, so maybe tester and manufacturer, i think it was it's first stamp.

  8. #8
    Join Date
    Oct 2014
    Posts
    2,135
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    Quote Originally Posted by Rondo View Post
    + sign followed by a star sign means test is good for 10 years. Most customer owned cylinders only get the +. I did a fair amount of hydrotesting back in the mid 80's
    All mine are customer owned and all do have + and the star

  9. #9
    Join Date
    May 2017
    Posts
    25
    Post Thanks / Like

    Re: Argon Tank Date Stamp Question

    Interesting post, thanks for the replies, Australia is probably different though

    Sent from my 5007U using Tapatalk

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,290,911.44585 seconds with 19 queries