    A friend just bought a brand new miller dynasty 280..its been running well for three weeks,then today has power input fault..and then pop!

    Have others had problems with the 280 ?
    I have a 200dx and its been ok (not as good as the Hitachi gp300 -last forever!)

  2. #2
    Join Date
    Nov 2014
    Location
    Southern CT
    Posts
    1,082
    Post Thanks / Like

    Re: dynasty 280

    Warranty time.
    Ernie F.

  3. Likes Lis2323 liked this post
  4. #3
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,610
    Post Thanks / Like

    Re: dynasty 280

    Good thing it was 3 weeks rather than 3 years. Certainly not a repair I would want to pay for.

  5. Likes metalman21 liked this post
  6. #4
    Join Date
    May 2007
    Posts
    4,589
    Post Thanks / Like

    Re: dynasty 280

    hopefully it was wired according to miller directions

  7. #5
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    4,233
    Post Thanks / Like

    Re: dynasty 280

    seen a few. with several different problems. does yours have the cooler power supply built into it? If so it might have failed.
    when they blow and the welder is out of warranty we don't fix the cooler power supply, just unplug it. replace pc7 and welder is usable.
    steal a line cord off a computer or monitor and plug the cooler into the wall. cooler runs all the time.
    At less the 1 month you might try taking it back where you bought it and see if they will contact Miller. and you might get a new welder.
    You can call miller tech support and tell them how old it is and what it did and see if you can arrange a replacement.
    Go to millerwelds.com first and register the welder. might have to upload a copy of the sales slip. Do first.

  8. Likes metalman21 liked this post
  9. #6
    Join Date
    Jul 2009
    Posts
    14
    Post Thanks / Like

    Re: dynasty 280

    Hi Thanks for that,will check.
    Even though its all well within warranty its not a good start.and not having a welder for a week while its being repaired is not good.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,273,671.94054 seconds with 19 queries