    Hi, Recently purchased a 180i. So far, I'm extremely pleased. Both my son and I can at least run continuous (sloppy) beads on scrap as we teach ourselves and practice. We've been using Lincoln Excalibur 7018, 3/32" rods.

    The current issue: We're going to weld some stiffeners on a mower deck. The mower is in the country and we'll be working off a generator. Portions of the 1/8" thick, 2"x2" angle iron stiffener have an small to maybe 3/16" gap to be filled/welded. Depending on how we can maneuver the mower deck the welding will be horizontal to almost overhead. We were planning on 6013 rods because we wanted light penetration of the existing deck, and fast freeze since approaching overhead is going to be a test of our ability. (Actually, it'll all be a test of our ability. But we want to give it a shot. )

    Any general suggestions?
    Any specific suggestions on a brand of 6013 rod that someone has had good success with using the 180I on 110 volts?

    Thanks. Florida Al

  2. #2
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,898
    Post Thanks / Like

    Re: best 6013 rod using 180i on 110 volts

    3/32" is a good size choice, and although I don't mind 6013, they are not a "fast-freeze" rod.

    3/32" or 1/8" 6011 are a very good choice for what you are doing.

    I would prefer 1/8" 6011 for this over 3/32" 6013.

    Both will run on the available amps with 120v input.

    Edit: as a bonus, 6011 rods have such light slag that repeated overlapping tacks or short overlapping beads are much easier to do.
    Last edited by MinnesotaDave; 08-11-2021 at 01:41 PM.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  3. #3
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,425
    Post Thanks / Like

    Re: best 6013 rod using 180i on 110 volts

    6011.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,355,272.27184 seconds with 11 queries