    I’ve got a 2016 vantage 520sd, used from United rentals with 4000 hours on it. Whenever I strike at arc on the back of the truck it is mounted to I get arc for about a second and then nothing. The lights on the machine blink and the read outs stop displaying numbers for a few seconds and then it returns to normal. I have not gotten ahold of Lincoln yet as it’s late in the day, just figured I would try my luck here. Thanks for your time.
    Last edited by BlackmountainW; 08-18-2021 at 11:03 PM. Reason: Typos

  2. #2
    Join Date
    Feb 2013
    Posts
    98
    Post Thanks / Like

    Re: Vantage 520sd output stops when welding on the back of my truck

    I have no idea but hopefully someone can help. Had a guy get mad because nobody answered his post but I don’t think these guys are getting paid to answer. Hopefully it’s a loose connection.

  3. #3
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    4,233
    Post Thanks / Like

    Re: Vantage 520sd output stops when welding on the back of my truck

    does it weld ok if you are on the ground and away from the truck. If so, welding current is getting into the welder controls and causing problems. Lincoln will need to know this. then they might be able to point you to a damaged filter or shorted wire. Also where are the weld leads, laid out on the ground with no coils or coiled up on top of the welder. Magnetic fields cause by the coils can cause problems with some welders. even coils on the ground.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,304,039.69283 seconds with 20 queries