    So recently, I was given an old (early 90s would be my guess) Ultraweld 130, DC inverter stick machine. Plugged into power, fan comes on, no weld. I can't find much info about it at all online. Hoping somebody may be able to offer some insight. Thanks

  2. #2
    Join Date
    Jul 2020
    Posts
    23
    Post Thanks / Like

    Re: Ultraweld 130 won't weld

    The UW130 does not have a built in gas valve so the use of a torch with a valve would be needed.

  3. #3
    Join Date
    Apr 2021
    Posts
    74
    Post Thanks / Like

    Re: Ultraweld 130 won't weld

    Quote Originally Posted by cpotter1112 View Post
    So recently, I was given an old (early 90s would be my guess) Ultraweld 130, DC inverter stick machine. Plugged into power, fan comes on, no weld. I can't find much info about it at all online. Hoping somebody may be able to offer some insight. Thanks
    I don't know the welder at all but I would open it up and see if it looks like the smoke has escaped. If it has, I suspect it would be cheaper to buy another.

    You might be lucky - have a peek.

    Jack

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,155,700.10330 seconds with 13 queries