Welding aluminum without a spoolgun
I just ran across a video of a guy mig welding aluminum with a old pipeline welding machine and a ln25 wire feeder i always thought you had to have a special set-up.
-
Re: Welding aluminum without a spoolgun
I've done a little aluminum when at the Ambulance, we had a little 120 vold Lincoln 140 mig, the 4043 wire didn't feed well, but the harder 5053 did better, keep the lead as traight as possible and learn to cuss till you get it down, it was just a slide out battery tray, it looked like crap, it was my first attempt at aluminum, but on the other side of the coin was the fact that it was still holding about 10 or 12 years later.
NRA LIFE MEMBER
UNITWELD 175 AMP 3 IN1 DC
MIDSTATES 300 AMP AC MACHINE
LET'S GO BRANDON!
"Those who would give up essential Liberty, to purchase a little temporary Safety, deserve neither Liberty nor Safety.” BENJAMIN FRANKLIN
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding aluminum without a spoolgun
All my welding in aluminum was with wire feeder.
Dave

Originally Posted by
Jwelder86
I just ran across a video of a guy mig welding aluminum with a old pipeline welding machine and a ln25 wire feeder i always thought you had to have a special set-up.
-
Re: Welding aluminum without a spoolgun
Looks almost like a cobra gun push/pull set up which is basically a big spoolgun imo.
Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.
-
Post Thanks / Like - 2 Likes, 0 Dislikes
-
Re: Welding aluminum without a spoolgun
There's mig welding AL and then there's mig welding AL......You will notice that there are no close-ups of welds. Heck, just about any feeder will splash weld AL. The outcome would likely have not been posted if he tried 4043 wire. This is the sort of vid I normally would have stopped after about 1 min. if that long. A guy yapping because he likes to hear himself yap.
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding aluminum without a spoolgun
There are a lot of variables in play here. The type/size wire, how long/straight the whip is, how effective the wire feeder is at pushing, etc. Spoolguns came about because aluminum wire is soft and doesn't feed reliably in many situations using a normal wire feeder...but it's not an absolute. I'm sure there are other folks welding aluminum with a normal wire feeder and whip, but they're probably being careful to keep the whip straight an only run 5056 wire (it's a bit stiffer).
While this method seems to have worked I wouldn't want to rely on it for anything other than occasional, or emergency use.
I will say that torch sure does look like a push/pull setup as N2 mentioned.
Check out my bench vise website:
http://mivise.com
Miller Syncrowave 250DX
Millermatic 350P with XR AlumaPro
Miller Regency 200 with 22A feeder and Spoolmatic 3
Hobart Champion Elite
Everlast PowerTig 210EXT
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding aluminum without a spoolgun
In the video he said it was just a regular straight gun that it wasn't a push pull gun
-
Re: Welding aluminum without a spoolgun
He showed the gun in the video and said its just a regular straight through gun
-
Re: Welding aluminum without a spoolgun
Push pull guns have the feed come in the back of the gun in line with the tip like this one he has. Regular guns have the feed come in the bottom of the grip.
-
Re: Welding aluminum without a spoolgun
https://www.mig-welding.co.uk/forum/...8/post-1833570
This is my Lorch S3, they have a perfect setup for welding aluminium without a pushpull or spoolgun. This configuration has no problems with 5356, 4043 or even pure 1050/1080 wire.
I was first put onto Lorch when we had huge problems with a Lincoln set trying to push pure 1050 wire through a 3m gun. We tried a push pull gun and it didn't work at all. The lorch dealer sent me a video of his S3 pushing 1080 wire though a 4m gun with a knot tied in the whip - no problems. I was literally sold.
Since then, I've bought both a Lorch TIG set and that S3 MIG set.
Push-pull guns are invaluable for bigger jobs like boats or trailer bodies etc where a 4m gun is impractical, I'd have one myself but I don't do enough large work to justify it. I also don't like spoolguns, the tiny reels of wire only last 5 minutes, plus, you get used to modern advanced pulse MIG setups with synchronised feeders for hot start/crater fill, double pulse etc. You don't get any of that on a spoolgun.
This way, all I do is change the liner, tip and driverolls to convert from steel wire to aluminium wire. It's cheap and very effective.
Last edited by Munkul; 09-06-2021 at 04:22 AM.
Murphy's Golden Rule: Whoever has the gold, makes the rules.
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding aluminum without a spoolgun
Thanks everyone for there input I'm going to message the guy and ask him for a better video and see what he tells me.
-
Re: Welding aluminum without a spoolgun

Originally Posted by
Jwelder86
Thanks everyone for there input I'm going to message the guy and ask him for a better video and see what he tells me.
The video is correct. There is no special set up needed for Alooominum.
You just need pure argon as the shielding gas and however you can get the AL wire delivered to the part yer working on, you are good to go.
That being said, some straight guns work better than others based on the wire feeder drive rolls.
Imma guess that dude in the video has some experience weldin' so he chose what works for him.
Weekend warriors like myself benefit from a Spoolgun set up as the chances of wire buggering up is eliminated 
AL is hard enough just trying to dial in the correct parameters to make a decent weld.
Ed Conley
http://www.screamingbroccoli.com/
MM252
MM211 (Sold)
Passport Plus & Spool gun
Lincoln SP135 Plus- (Gone to a good home)
Klutch 120v Plasma cutter
SO 2020 bender
Beer in the fridge
-
Re: Welding aluminum without a spoolgun
Years ago a member posted his aluminum welding without a spool gun
. imgineer was the member. There have been others.
However, i think dude in the video is cheating. I think his gun is pulling. Judging be zero regard for cable straightness.
Straight cables is consistent parameter amongst those using plain wire feeders. Short whips help too.
-
Re: Welding aluminum without a spoolgun

Originally Posted by
Munkul
The Lorch dealer sent me a video of his S3 pushing 1080 wire though a 4m gun with a knot tied in the whip - no problems. I was literally sold.
This is what I say to people who insist that you have to keep the whip straight.
You just need a slicker feed setup
Murphy's Golden Rule: Whoever has the gold, makes the rules.
-
Re: Welding aluminum without a spoolgun

Originally Posted by
Munkul
This is what I say to people who insist that you have to keep the whip straight.
You just need a slicker feed setup

Thanks. I guess the harder wire, 1\16 liner and straight gun were the slicker set up. Otherwise he says everything was "plain jane". 2 of those variables are not common in small home shops.
-
Re: Welding aluminum without a spoolgun
Does anybody else have a straight gun like that is not push-pull? Why is it desired? Looks like it would be unnecessarily bulky for general use?
-
Re: Welding aluminum without a spoolgun

Originally Posted by
Jwelder86
Thanks everyone for there input I'm going to message the guy and ask him for a better video and see what he tells me.
Thought you might have tried this already.
Teflon liners are about $30 , still cheaper than a spoon gun, and spool guns are far cheaper than a LN25.
What kind of welding machine do you have ?
Airco 250 ac/dc Heliwelder Square wave
Miller Synchrowave 180 sd
Miller Econo Twin HF
Lincoln 210 MP
Dayton 225 ac/dc
Victor torches
Snap-On YA-212
Lotos Cut60D
Primeweld 225 ac/dc
Primeweld mig180
Miller AEAD-200
-
Re: Welding aluminum without a spoolgun
Hey guy the realistic welder finally made the video I asked about months ago about the gun he was using.
-
Re: Welding aluminum without a spoolgun
-
Re: Welding aluminum without a spoolgun
The pistol grip gun just lets the wire shoot straight through the cable without the bend in the gooseneck of a regular gun However, It's amazing what you can do with aluminum with a 4 wheel drive feed system. Even more what you can do with 4 wheel drive and Python push pull. If not for that, the teflon or nylon liners with U groove drive rolls, Regular 10' gun with 45 degree gooseneck and a little experience can solve the spoolgun problem. That being said, $200 for a 24v spoolgun with a simple hookup diagram can solve some problems as well. Pick your poison.
Last edited by Rondo; 02-25-2022 at 08:50 PM.
Thermal Arc 320SP ( Lorch )
Cobra Pythons
Thermal Arc 300 AC/DC ( Sanrex )
ESAB 301i AC/DC ( Lorch )
Thermal Arc 161STL ( WTL )
Thermal Arc 190S ( Sanrex )
Cut Master 82, 42. Cut45 ( WTL )
Victor Gas Apps.
Boxes and boxes of welding crap.
-
Re: Welding aluminum without a spoolgun
It more of keeping the gun cable straight and short about 6 to 10 feet.
The tension on feed needs to be very low.
Dave

Originally Posted by
Jwelder86
Hey guy the realistic welder finally made the video I asked about months ago about the gun he was using.
-
Re: Welding aluminum without a spoolgun
That mig gun is for large diameter wire it looks like a 400 amp tweco .
I had one that size for welding steel I also had Miller 750 amp too.
Four wheel drive is also for large wire it does not do to much for for small aluminum wire.
A simple single drive will work great for small size wire. A standard mig gun will do a good job. 👍
Dave

Originally Posted by
Jwelder86