    I'm new to this and have a question...

    I'm joining two parts with two or three plug welds. The top part (with the plug holes) is 2" wide, 3" long 3/16" flat bar. The bottom part is a 6" long 3/8" square bar. If I drill divots into the bottom part where the plug welds will be, will that make them stronger? Or is there any other prep (besides cleaning) that will make for a stronger weld?

  2. #2
    Join Date
    Sep 2012
    Location
    Wheatland, Wyoming
    Posts
    468
    Post Thanks / Like

    Re: Plug welds

    What size holes? What welding process?
    Chris
    Auction Addict

  3. #3
    Join Date
    Dec 2018
    Posts
    5,840
    Post Thanks / Like

    Re: Plug welds

    Your plug welds will be no stronger than the square inches of weld contacting the 3/16 around the perimeter of the hole in that plate. Drilling deeper into the 3/8 gives no additional strength to the assembly. Welds are sized/spec'd taking into account just how much of the weld contacts the parent metal. Small contact area, less strength. The weak link is the steel itself.

  4. #4
    Join Date
    Dec 2008
    Posts
    58
    Post Thanks / Like

    Re: Plug welds

    So the bigger the plug welds the better?

    Holes are currently 1/4", process is flux-core.

  5. Likes walker liked this post
  6. #5
    Join Date
    Feb 2015
    Posts
    132
    Post Thanks / Like

    Re: Plug welds

    Quote Originally Posted by upand_at_them View Post
    So the bigger the plug welds the better?

    Holes are currently 1/4", process is flux-core.


    There is nothing wrong with what you are trying to do. I am only referring to your plan of utilizing plug welds to join two pieces of steel. There is, however, a "fly in the ointment". That is your 1/4 inch holes. They need to be larger. They are too small.
    And it is "arc force" that will provide your divot. That's one way of describing it at least.

    Sent from my E6810 using http://tiny.cc/Forums_reader

  7. #6
    Join Date
    Dec 2008
    Posts
    58
    Post Thanks / Like

    Re: Plug welds

    Okay, then I'll make the holes as large as the bar being joined: 3/8", or maybe just 23/64".

    By the way, the plug welds won't be the only welds joining the two pieces. I'll also be laying beads on the other side. I just wanted the fullest join since I'll be stressing the 3/8" bar and don't want it to break free.

  8. #7
    Join Date
    Feb 2015
    Posts
    132
    Post Thanks / Like

    Re: Plug welds

    Quote Originally Posted by upand_at_them View Post
    Okay, then I'll make the holes as large as the bar being joined: 3/8", or maybe just 23/64".

    By the way, the plug welds won't be the only welds joining the two pieces. I'll also be laying beads on the other side. I just wanted the fullest join since I'll be stressing the 3/8" bar and don't want it to break free.


    I seriously doubt you will achieve your goal even with a 3/8 hole. At least with the type of equipment I suspect you are using. I would recommend a 3/4 hole as the smallest size that may be effective.

    Sent from my E6810 using http://tiny.cc/Forums_reader

  9. #8
    Join Date
    Dec 2008
    Posts
    58
    Post Thanks / Like

    Re: Plug welds

    But a 3/4" hole is better than the 3/8" material being welded to.

  10. #9
    Join Date
    Jul 2008
    Posts
    3,095
    Post Thanks / Like

    Re: Plug welds

    What are you making that requires such Godawful strength? Assuming you're using A36 mild steel (yield strength 36ksi), each 3/8" plug weld is gonna require nearly 3/4 ton of force to yield. Now multiply that by how many plug welds you're making.

    In my experience, overwelding -- and the warping and distortion that go with it -- is a much more common problem than insufficient strength. Steel is stronger than you probably realize.

    You might want to estimate your expected maximum loads before overwelding and then having to cut it all apart and re-do it (with fewer welds) because it twisted up like a pretzel...

  11. #10
    Join Date
    Sep 2012
    Location
    Wheatland, Wyoming
    Posts
    468
    Post Thanks / Like

    Re: Plug welds

    Quote Originally Posted by upand_at_them View Post
    Okay, then I'll make the holes as large as the bar being joined: 3/8", or maybe just 23/64".

    By the way, the plug welds won't be the only welds joining the two pieces. I'll also be laying beads on the other side. I just wanted the fullest join since I'll be stressing the 3/8" bar and don't want it to break free.
    Then you do not need plug welds. The welds on the other side will be all you need.
    Chris
    Auction Addict

  12. #11
    Join Date
    Dec 2008
    Posts
    58
    Post Thanks / Like

    Re: Plug welds

    Here's what I did. No plug welds. It's part of a small metal bender, for 16 gauge bar. I wound up using a 1/2" round for the handle.

    It's hard to tell due to sitting on a stone wall, but I had a little burn in at the end of the welds (bottom right and top left). I was working with my backup (handheld) shield as my auto-dark helmet died. Otherwise I'm fairly satisfied with how well they're joined.

    Name:  IMAG1355.jpg
Views: 122
Size:  74.1 KB

  13. #12
    Join Date
    Aug 2012
    Location
    AR
    Posts
    2,074
    Post Thanks / Like

    Re: Plug welds

    Your biggest problem with plug welds will be slag inclusions and porosity......those small holes will be more like tack welds at best.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,634,842,589.53673 seconds with 14 queries