    Plenum repair

    Any of you guys have done a plenum repair on a car? I need to graft a donor piece into my rusted out plenum.Name:  20210821_111028-min.jpg
Views: 650
Size:  141.8 KBName:  20210919_131536.jpg
Views: 620
Size:  111.2 KBName:  653844618.jpg
Views: 623
Size:  255.4 KB

  2. #2
    Join Date
    Jun 2016
    Posts
    1,002
    Post Thanks / Like

    Re: Plenum repair

    get your replacement part first and look at it and see which way is the easiest to fit and trim it to yours.
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  3. #3
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Plenum repair

    You can't weld in a replacement unless it reaches beyond the rusted out area. I have concern you will have to attempt some portion on rusted out stuff, that won't work.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  4. #4
    Join Date
    Apr 2016
    Location
    CA
    Posts
    12,117
    Post Thanks / Like

    Re: Plenum repair

    240/260z ?
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  5. #5
    Join Date
    Apr 2016
    Posts
    570
    Post Thanks / Like

    Re: Plenum repair

    Quote Originally Posted by duramax-rob View Post
    get your replacement part first and look at it and see which way is the easiest to fit and trim it to yours.
    I think the third photo is the replacement?

  6. #6
    Join Date
    Jun 2016
    Posts
    1,002
    Post Thanks / Like

    Re: Plenum repair

    might want to replace it at windshield post and rocker and make panels to cover rest of floor. and any other rusted out parts on replacement part. might be easier also. if it is a datson z those were rust buckets.
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  7. #7
    Join Date
    May 2010
    Posts
    88
    Post Thanks / Like

    Re: Plenum repair

    I was thinking of tacking the donor to the vertical piece in front of the windshield pinch weld. Only problem is I dont see how I can get that seam water tight. Even brazed I think water could get in the seam. Water would get into the plenum which is no biggie, just a rusted joint issue.Name:  donor (2).jpg
Views: 383
Size:  140.7 KBName:  old pinch.jpg
Views: 381
Size:  115.5 KB

  8. #8
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Plenum repair

    If you can get to clean material where the weld will be free of rust; choose your cuts. I want a butt weld everywhere, except where the manufacturer used an overlap with spot welds. There, drill out the spot welds.
    Take your time, use progressively more precise tools to cut. Your goal is to have a fit with a hair width or less.
    I'd then be torn between a gas weld & a TIG weld on steel butt welds of 20 gauge or so.

    Again, if you hope to weld rust, all bets are off.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  9. #9
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,975
    Post Thanks / Like

    Re: Plenum repair

    Sealing isn't a big issue. The big question is how much you have to replace to be working with all good metal again. If you need to seal it up after spot welding, you can coat the gap with 3-M seam sealer or give it a layer of fiberglass if it isn't visible after assembly. If it does show, go over the fiberglass with a skim coat of bondo and finish as you would any other body work. That's a uni-body car. The rust isn't just affecting appearance, it's affecting the strength and integrity of your car's chassis... keep that in mind when inspecting it for rusted components.
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  10. #10
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Plenum repair

    Quote Originally Posted by whtbaron View Post
    Sealing isn't a big issue. The big question is how much you have to replace to be working with all good metal again. If you need to seal it up after spot welding, you can coat the gap with 3-M seam sealer or give it a layer of fiberglass if it isn't visible after assembly. If it does show, go over the fiberglass with a skim coat of bondo and finish as you would any other body work. That's a uni-body car. The rust isn't just affecting appearance, it's affecting the strength and integrity of your car's chassis... keep that in mind when inspecting it for rusted components.
    & don't be afraid to put a backer plate behind a particular strength important joint. You can successfully weld a wider gap with a 2" wide backer plate on the side you can't see. Still don't want a sheet metal butt joint more than 3/32". First drill a series of holes in body metal along the edges of the backer to plug weld there. Be thorough with the seam sealer to keep water out.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  11. #11
    Join Date
    Jun 2016
    Posts
    1,002
    Post Thanks / Like

    Re: Plenum repair

    you will have to butt weld the joint where you think you will have a sealing problem area. that to ensure that you have the same thickness uniformity as original. like where the windshield sits but just below you can lap weld or butt weld with backer plate.
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  12. #12
    Join Date
    May 2010
    Posts
    88
    Post Thanks / Like

    Re: Plenum repair

    Its really a tricky proposition. This is not a 57 chevy where you can buy every part. This is a rusty jap car, plenum not available. In a perfect world i would replace the whole plenum but......the pinch weld is perfect and its acting like a tie beam. So i was thinking of putting the complete donor plenum over the existing plenum. Sounds dumb but i think it could work and be strong.

  13. #13
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Plenum repair

    Quote Originally Posted by johnfin View Post
    Its really a tricky proposition. This is not a 57 chevy where you can buy every part. This is a rusty jap car, plenum not available. In a perfect world i would replace the whole plenum but......the pinch weld is perfect and its acting like a tie beam. So i was thinking of putting the complete donor plenum over the existing plenum. Sounds dumb but i think it could work and be strong.
    You really need to blast clean this mess to see what is left that you could actually weld to.

  14. Likes whtbaron liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,280,711.64644 seconds with 22 queries