    coffe table from square tubing.

    Heres my last project.
    Wanted to make a kind of rustic looking coffe table. Since I was not able to avoid grinding, I had to paint it, so it did not come out that rustic any more, but still.. not a bad table in my opinion.
    Name:  IMG_20210929_190209_resized_20211004_095107056.jpg
Views: 844
Size:  97.3 KB
    Name:  IMG_20210929_190225_resized_20211004_095107268.jpg
Views: 798
Size:  52.8 KB
    Name:  IMG_20210929_190142_resized_20211004_095106809.jpg
Views: 786
Size:  152.4 KB
    Name:  IMG_20211001_203157_edit_618242290779620_resized_20211004_095208120.jpg
Views: 781
Size:  107.5 KB

    Name:  IMG_20211001_203211_resized_20211004_095208680.jpg
Views: 778
Size:  52.3 KB

  2. #2
    Join Date
    Dec 2008
    Posts
    116
    Post Thanks / Like

    Re: coffe table from square tubing.

    Krikey! Coffee table for Zeus? Nice simple design, but don't expect the wife to lift that.

  3. Likes farmersammm liked this post
  4. #3
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: coffe table from square tubing.

    Nice looking table, really nice. I like the distressed edges.

  5. #4
    Join Date
    Dec 2014
    Location
    Northern California
    Posts
    542
    Post Thanks / Like

    Re: coffe table from square tubing.

    I like the gussets for strength!

    OP…nice build and I guess steel don’t cost as much where you are cause that looks expensive and that looks strong enough to work as a HD workbench as well….

  6. #5
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,295
    Post Thanks / Like

    Re: coffe table from square tubing.

    Good job, nice design, and great project.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  7. #6
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,896
    Post Thanks / Like

    Re: coffe table from square tubing.

    Looks great 👍
    Steel will last a long time

    Dave

    Quote Originally Posted by krl View Post
    Heres my last project.
    Wanted to make a kind of rustic looking coffe table. Since I was not able to avoid grinding, I had to paint it, so it did not come out that rustic any more, but still.. not a bad table in my opinion.
    Name:  IMG_20210929_190209_resized_20211004_095107056.jpg
Views: 844
Size:  97.3 KB
    Name:  IMG_20210929_190225_resized_20211004_095107268.jpg
Views: 798
Size:  52.8 KB
    Name:  IMG_20210929_190142_resized_20211004_095106809.jpg
Views: 786
Size:  152.4 KB
    Name:  IMG_20211001_203157_edit_618242290779620_resized_20211004_095208120.jpg
Views: 781
Size:  107.5 KB

    Name:  IMG_20211001_203211_resized_20211004_095208680.jpg
Views: 778
Size:  52.3 KB

  8. #7
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,977
    Post Thanks / Like

    Re: coffe table from square tubing.

    Looks great... but just how big are your coffee cups??
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  9. #8
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: coffe table from square tubing.

    Name:  271189-Here-Is-Your-Cup-Of-Coffee.jpg
Views: 734
Size:  47.9 KB

  10. Likes Reebz, whtbaron liked this post
  11. #9
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,478
    Post Thanks / Like

    Re: coffe table from square tubing.

    You need a "sofa" to go with the coffee table, 2" x 1/4" angle, 1" solid round steel bars, steel wheels,, Composite boards, and LOTS of stainless bolts!!




  12. Likes whtbaron, scsmith42 liked this post
  13. #10
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,896
    Post Thanks / Like

    Re: coffe table from square tubing.

    Finally the right size coffee cup.

    Dave

    Quote Originally Posted by farmersammm View Post
    Name:  271189-Here-Is-Your-Cup-Of-Coffee.jpg
Views: 734
Size:  47.9 KB

  14. #11
    Join Date
    Jun 2009
    Location
    Draper, UT
    Posts
    505
    Post Thanks / Like

    Re: coffe table from square tubing.

    Nice work,

    I tend to go lighter weight and use 12x24 floor tiles for the tops and shelves

    Name:  20161211_153103.jpg
Views: 735
Size:  63.4 KB

    Name:  20180722_080326.jpg
Views: 695
Size:  241.9 KB
    MillerMatic 252, HTP 221 w/cooler, Hypertherm PM45, Lincoln IdealArc 250 AC/DC, victor Oxy/Acet

    "I'd like to believe as many true things and as few false things as possible"

  15. Likes whtbaron liked this post
  16. #12
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    575
    Post Thanks / Like

    Re: coffe table from square tubing.

    Love the table. I have made a few like that. In event of tornado get under that.

  17. #13
    Join Date
    Feb 2021
    Posts
    38
    Post Thanks / Like

    Re: coffe table from square tubing.

    Quote Originally Posted by Tarmstrong View Post
    I like the gussets for strength!

    OP…nice build and I guess steel don’t cost as much where you are cause that looks expensive and that looks strong enough to work as a HD workbench as well….

    Steel(and also wood) is still expensive. But since this build was more for the fun of building suff, its not that bad. Fot the cost of the material(bought in small qty`s) i could have for sure bought the most expensive coffe table from IKEA.


    And the gussets.. these are just for the bolt to go through, to hold the table top.

  18. #14
    Join Date
    Feb 2021
    Posts
    38
    Post Thanks / Like

    Re: coffe table from square tubing.

    I also made holes in the endplates of legs, with a M16 nut welded on the inside, so the table could be leveled(probably couple of mm adjustment is needed) with M16 bolts. But I need to find some sort of plastic caps for the bolts, so it does not scratch the floor.
    Something like this:
    Name:  M16 caps.jpg
Views: 672
Size:  15.7 KB
    Last edited by krl; 10-05-2021 at 02:54 AM.

  19. #15
    Join Date
    Dec 2016
    Location
    New Jersey
    Posts
    405
    Post Thanks / Like

    Re: coffe table from square tubing.

    Nice looking table. Well executed, symmetrical - sturdy as heck! I like it.

  20. #16
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,478
    Post Thanks / Like

    Re: coffe table from square tubing.

    Quote Originally Posted by krl View Post
    I also made holes in the endplates of legs, with a M16 nut welded on the inside, so the table could be leveled(probably couple of mm adjustment is needed) with M16 bolts. But I need to find some sort of plastic caps for the bolts, so it does not scratch the floor.
    Something like this:
    Name:  M16 caps.jpg
Views: 672
Size:  15.7 KB
    Our local Walmart carries Plasti-Dip spray that would coat those bolt heads with a thick scratch resistant coating,, for $6,,,


  21. #17
    Join Date
    Aug 2014
    Location
    BC Canada
    Posts
    14,716
    Post Thanks / Like

    Re: coffe table from square tubing.

    Quote Originally Posted by SweetMK View Post
    Our local Walmart carries Plasti-Dip spray that would coat those bolt heads with a thick scratch resistant coating,, for $6,,,

    I like the Plasti-Dip idea.


    I made levellers using heavy washers and 5/8” bolts for this lathe stand. A round felt pad could be glued to the underside (perhaps)

    That may also work for your industrial look.





    Sent from my iPad using Tapatalk
    :

  22. Likes SweetMK liked this post
  23. #18
    Join Date
    Feb 2021
    Posts
    38
    Post Thanks / Like

    Re: coffe table from square tubing.

    I have been welding nuts on the bottom(inside) of everything lately to make things adjustable. I have mada a bunch of silimary styled stools also, but for these a standard M8 leveling things work fine.
    Name:  IMG_20211005_183639.jpg
Views: 632
Size:  267.5 KBName:  IMG_20211005_183656.jpg
Views: 635
Size:  381.9 KB

  24. Likes psacustomcreations, SweetMK liked this post
  25. #19
    Join Date
    Aug 2014
    Location
    BC Canada
    Posts
    14,716
    Post Thanks / Like

    coffe table from square tubing.

    Quote Originally Posted by krl View Post
    I have been welding nuts on the bottom(inside) of everything lately to make things adjustable. I have mada a bunch of silimary styled stools also, but for these a standard M8 leveling things work fine.
    Name:  IMG_20211005_183639.jpg
Views: 632
Size:  267.5 KBName:  IMG_20211005_183656.jpg
Views: 635
Size:  381.9 KB
    The bottoms of those stool legs are nicely finished.

    Great attention to detail


    Sent from my iPad using Tapatalk
    :

  26. #20
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    939
    Post Thanks / Like

    Re: coffe table from square tubing.

    I would recommend against plasti-dip for this as it is vinyl and will leach plasticizers and leave marks on surfaces. You want either teflon or HDPE or possibly PP plastic caps for this so they don't leave marks and are soft enough not to scratch.

    And nice work!
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  27. Likes Lis2323 liked this post
  28. #21
    Join Date
    Dec 2008
    Posts
    116
    Post Thanks / Like

    Re: coffe table from square tubing.

    Felt?

  29. #22
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,295
    Post Thanks / Like

    Re: coffe table from square tubing.

    Quote Originally Posted by frieed View Post
    Nice work,

    I tend to go lighter weight and use 12x24 floor tiles for the tops and shelves

    Name:  20161211_153103.jpg
Views: 735
Size:  63.4 KB


    Name:  20180722_080326.jpg
Views: 695
Size:  241.9 KB

    I’m interested in how you support the tiles. Is it solid under the tiles or straps?

    Are the tiles flush on top with the steel or are they under the steel?
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  30. #23
    Join Date
    Jun 2009
    Location
    Draper, UT
    Posts
    505
    Post Thanks / Like

    Re: coffe table from square tubing.

    I use some flat bar to support the tops and make them flush with the tube.
    The lower shelves have two tiles double stacked for ballast.

    Name:  20180721_131457.jpg
Views: 522
Size:  226.2 KB
    MillerMatic 252, HTP 221 w/cooler, Hypertherm PM45, Lincoln IdealArc 250 AC/DC, victor Oxy/Acet

    "I'd like to believe as many true things and as few false things as possible"

  31. Likes wb4rt liked this post
  32. #24
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,180
    Post Thanks / Like

    Re: coffe table from square tubing.

    Those tables really look good. Another take on them would be to leave a slot down the middle for a trash tray. As you're preparing food, the scraps get scraped into a drawer that you empty later. I've made several for people out of their granite sink cut outs.
    Attached Images Attached Images   

  33. #25
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: coffe table from square tubing.

    Quote Originally Posted by krl View Post
    Heres my last project.
    Wanted to make a kind of rustic looking coffe table. Since I was not able to avoid grinding, I had to paint it, so it did not come out that rustic any more, but still.. not a bad table in my opinion.
    Name:  IMG_20210929_190209_resized_20211004_095107056.jpg
Views: 844
Size:  97.3 KB
    Name:  IMG_20210929_190225_resized_20211004_095107268.jpg
Views: 798
Size:  52.8 KB
    Name:  IMG_20210929_190142_resized_20211004_095106809.jpg
Views: 786
Size:  152.4 KB
    Name:  IMG_20211001_203157_edit_618242290779620_resized_20211004_095208120.jpg
Views: 781
Size:  107.5 KB

    Name:  IMG_20211001_203211_resized_20211004_095208680.jpg
Views: 778
Size:  52.3 KB


    The Base looks GREAT.

    But it needs a better looking top and bottom shelf.

    sorry if that was mentioned before... I didn't read the other replies.

    My opinion is the only one that matters.

    Keep up the good work.

    John T.
    - The voice of reason.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,287,246.10305 seconds with 20 queries