    I Might of Really Stepped In It.

    I got to thinking about that damn pipe I got, and why it would be threaded, and have couplings on one end.

    I'm thinkin' this crap might be casing.

    Got so upset about it, I went out and looked at it on the trailer.

    Plain as day........................it's labeled J55

    Based on what I've been able to come up with...........................................it' s not suitable for welding because of the high carbon content.

    https://www.worldironsteel.com/news/...-25170138.html

    .34-.39 carbon content. I'm pretty sure this is a disaster waiting to happen.

    Luckily, it's still on the trailer.
    Last edited by farmersammm; 10-13-2021 at 04:04 AM. Reason: bad link

  2. Likes whtbaron, John Baptist liked this post

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,300,626.89218 seconds with 21 queries