    Help needed powcon 400smt

    Ok so this is the story guy had this listed for 200$ on offerup had 3 phase plug on it. Told him that without seeing it power up i was willing to do 175$ A steal (i thought) so i picked it up cut the plug off and followed the directions on the underside of the case rotated circuit board 180 so that 230v was on the top removed brass buss bar that connected 3and4 and moved it to 1 and 2 and added buss bar to 3 and 4 droped the red wire on breaker/on off switch and isolated it. Now i plug in and when i flip the breaker to on it comes on very briefly with a strange noise then kicks off not sure if this is a capacitor issue possibly a on off breaker if anyone is familar with these machines or has had this issue i could use some knowledge i hate going down the rabbit hole

    Cheers justin

  2. #2
    Join Date
    Oct 2021
    Posts
    8
    Post Thanks / Like

    Re: Help needed powcon 400smt

    Problem identified all it took was tearing it down to find it capacitor negative was so corroded it was actually not even connected and the capacitor was Shot 2 easy fix.Name:  20211023_124345.jpg
Views: 39
Size:  60.9 KB
    Attached Images Attached Images  

  3. #3
    Join Date
    Oct 2021
    Posts
    8
    Post Thanks / Like

    Re: Help needed powcon 400smt

    Problem identified all it took was tearing it down to find it capacitor negative was so corroded it was actually not even connected and the capacitor was Shot 2 easy fix.Name:  20211023_124345.jpg
Views: 39
Size:  60.9 KBName:  20211023_124355.jpg
Views: 39
Size:  51.5 KB

  4. #4
    Join Date
    Apr 2019
    Posts
    18
    Post Thanks / Like

    Re: Help needed powcon 400smt

    Hi Justin. Glad you were able to find the problem, and thanks for sharing!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,640,956.36668 seconds with 12 queries