    Just wondering has anyone ever removed the axle tube mounts from the top of the axle and re-welded them on the bottom to switch from over slung to under slung? Or would you just weld on a new set and leave the other ones?

    Thanks.
    Millermatic 211
    Lincoln Precision TIG 225
    Century 250 MIG
    Lincoln 225 AC Box (sold)


    I support my local welding store (Amazon, McMasterCarr, Cyberweld, EBay).

  2. #2
    Join Date
    Dec 2008
    Location
    Lockhart,Tx (BBQ capitol of the world)
    Posts
    1,204
    Post Thanks / Like

    Re: 3500# Trailer Axle Modification

    I have cut them off an repositioned them and after I was finished I decided I would never do that again!
    The new ones are too cheap!
    Last edited by rexcormack; 10-28-2021 at 09:52 AM. Reason: spelling

  3. Likes fixit32068 liked this post
  4. #3
    Join Date
    Apr 2006
    Location
    S.E.Wisc.
    Posts
    157
    Post Thanks / Like

    Re: 3500# Trailer Axle Modification

    I added new ones and left the old mounts when I wanted to lower a motorcycle trailer.

  5. Likes fixit32068 liked this post
  6. #4
    Join Date
    Jan 2012
    Posts
    168
    Post Thanks / Like

    Re: 3500# Trailer Axle Modification

    Thanks. I decided to flip the axles since they are straight axles with camber. I have to lengthen the axles anyway. I will remove the camber when I do it. I don't like cambered axles and the added bigger diameter center piece will stiffen it up. This is a low use trailer so I'm not worried about tire wear either.
    Millermatic 211
    Lincoln Precision TIG 225
    Century 250 MIG
    Lincoln 225 AC Box (sold)


    I support my local welding store (Amazon, McMasterCarr, Cyberweld, EBay).

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,834,138.36791 seconds with 14 queries