Let me preface this by saying I don’t stick weld often.

I can do it, i know what a good sound weld looks like but I’m not being featured in any magazines…

That said, i have to cut this tower up, relocate it and put it back together.

I’d like to use 6013 because I just know I’ll make cleaner welds with it.

So that said, am i taking a risk on strength using 6013 to get nicer welds or is it a non concern in the application?

This tower is 6x6 3/16 wall tube. So it’s going have a good 24” of weld on each section.

Also, this thing is a death trap as it sits welding wise and has held up for 10+ years. No idea what hack did it the first time around. It’s got one weld on each piece…

This is a rope training tower and is being relocated to my current firehouse where I’m building the attached training center.

Oh and I hope everyone’s doing well, haven’t been around much

Name:  3D270EAF-83CB-4DFE-9525-AB19B0817436.jpg
Views: 1940
Size:  350.6 KBName:  0FA116EA-72BD-4F72-8966-737F032A9E99.jpg
Views: 1913
Size:  239.2 KBName:  5F778403-1DBE-4383-A9E1-CEC63F27A563.jpg
Views: 1905
Size:  152.2 KBName:  0FFB0FBC-07E4-49DE-8B68-1F1E05C854A5.jpg
Views: 1889
Size:  71.6 KBName:  C35E767E-0766-4A04-B333-E321A32AFE71.jpg
Views: 1870
Size:  70.2 KB