    So i bought this machine off anazon. 220v 50 amp 85% duty cycle and it only makes a 2 inch cut thru thin sheet metal then stops. I can start it again but its a hassle. Does plasma have issues going thru rusty metal. Dissapointed, i thing its going back. Zero customer service.

  2. #2
    Join Date
    Dec 2013
    Posts
    2,358
    Post Thanks / Like

    Re: Amico 50hf plasma issues

    They will do that if you don't have a good ground/work lead connection on whatever you are cutting. Could be some thing else too.
    ---Meltedmetal

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,311,190.05438 seconds with 20 queries