    What kind of metal?

    It's heavy. Cast iron of some flavor?
    Attached Images Attached Images  

  2. #2
    Join Date
    Sep 2012
    Location
    Wheatland, Wyoming
    Posts
    600
    Post Thanks / Like

    Re: What kind of metal?

    Drill into it with an 1/8" drill bit about an 1/8". If the cuttings are granular it is likely cast iron.
    Chris
    Auction Addict

  3. #3
    Join Date
    Jun 2017
    Posts
    141
    Post Thanks / Like

    Re: What kind of metal?

    Quote Originally Posted by tiggen View Post
    It's heavy. Cast iron of some flavor?
    It’s a meteorite…worth 100,000


    Sent from my iPhone using Tapatalk Pro

  4. #4
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,642
    Post Thanks / Like

    Re: What kind of metal?

    Miller Multimatic 255

  5. #5
    Join Date
    Dec 2013
    Posts
    1,916
    Post Thanks / Like

    Re: What kind of metal?

    What it was part of will often give you clues to the most likely suspected alloy.
    ---Meltedmetal

  6. #6
    Join Date
    Jun 2019
    Location
    Atlanta, GA
    Posts
    31
    Post Thanks / Like

    Re: What kind of metal?

    It came off a rabbit, the kind of thing my mother in law would have in her garden. It is a solid casting, which I find odd. Most of these lawn ornaments I've seen are hollow. She wanted to know if I could weld it back on. Will do spark and drill test if she brings it back.

  7. #7
    Join Date
    Dec 2013
    Posts
    1,916
    Post Thanks / Like

    Re: What kind of metal?

    Then if it is iron (magnetic) it is most likely gray iron of whatever grade was in the furnace the day they wanted to get the molds off the pouring floor. Up here it would get o/a brazed and painted. Or if the bronze was going to offend someone maybe welded with cast iron again with o/a.
    ---Meltedmetal

  8. #8
    Join Date
    Oct 2014
    Posts
    3,854
    Post Thanks / Like

    Re: What kind of metal?

    I'd probably just use an epoxy to repair a lawn ornament. It's has a lot of rough surface area so should work great and keep the existing colour match.

  9. Likes 12V71, wb4rt, CAVEMANN, whtbaron liked this post
  10. #9
    Join Date
    May 2011
    Posts
    548
    Post Thanks / Like

    Re: What kind of metal?

    Epoxy

    If you weld it, that kind of stuff is made with pot metal. Like anything around the pot gets dropped into it, steel, other cast, aluminum, the older Chinese guy who wanted a raise.... anything.

    Sent from my SM-G960U using Tapatalk

  11. Likes 12V71 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,643,043,453.16386 seconds with 15 queries