    Crawler007's random welding projects

    Hi All,

    Thought I would share some of my projects here, I just like to build stuff and most of the time it's project's for me so not making money at this (actually costing myself money lol) its all in fun. So please don't take any of this to serious, I sure don't!

    Well I bought a new to me 50yr old mill and decided to try a small firts project so I came up with this, I still have a brass weight to add to the pointer but its 90% finished.


    Name:  3rd hand 1.jpg
Views: 1414
Size:  114.9 KBName:  3rd hand 2.jpg
Views: 1421
Size:  112.7 KBName:  3rd hand 3.jpg
Views: 1415
Size:  95.2 KBName:  3rd hand 4.jpg
Views: 1414
Size:  109.7 KBName:  3rd hand 5.jpg
Views: 1404
Size:  98.5 KB

  2. #2
    Join Date
    Jul 2021
    Location
    Pitman PA
    Posts
    222
    Post Thanks / Like

    Re: Crawler007's random welding projects

    What is this?

  3. Likes 12V71 liked this post
  4. #3
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,295
    Post Thanks / Like

    Re: Crawler007's random welding projects

    That's pretty cool, at first I thought you were making a hammer. Lol

  5. #4
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,051
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by old miner called Pop View Post
    What is this?
    I was eyeing up that hammer looking part too... my best guess is a third hand to hold things down while he's welding..
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  6. #5
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    706
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Yes, I would say a third hand welding thingy too. At first I thought it was a stand for a dial indicator.
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  7. Likes whtbaron liked this post
  8. #6
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Yep welding thrirdhand, unnecessary joint and replaceable pointer, but was just really wanting to build somthing with the lathe and mill.

  9. #7
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,779
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Very nice..

    Nothing like mill or lathe to help us spend 10x the time making tools.

    I understand...

  10. #8
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,257
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by old miner called Pop View Post
    What is this?
    Tig welders third hand. Very nice one!

  11. Likes Lis2323 liked this post
  12. #9
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,326
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Extremely nice!


    Better than mine …




    Sent from my iPad using Tapatalk
    :

  13. #10
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    706
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Boooo!! C'mon Terry - it's Christmas time now, not Halloween!
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  14. Likes Lis2323 liked this post
  15. #11
    Join Date
    May 2021
    Location
    45.97267, -106.27818
    Posts
    419
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by tapwelder View Post
    Very nice..

    Nothing like mill or lathe to help us spend 10x the time making tools.

    I understand...
    Better than spending 10x the money for a tool not worth it's price.

  16. Likes N2 Welding liked this post
  17. #12
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,779
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Did you make a tool to radius the ends? Looks like you practiced a lot of techniques on your mill.
    Last edited by tapwelder; 12-05-2021 at 07:45 AM.

  18. #13
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,762
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by old miner called Pop View Post
    What is this?
    It's a fancy "third hand"

    you know, one of the first welding projects you make.....

    Then it sits on a shelf forever, never used.

    looks cool though.



    waiting for the comments.... "I use mine all the time"

    In the real world you just grab whatevers handy to prop something up. Or tack something and grind it off later.....

    Get IT Done
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  19. Likes _Weldman_ liked this post
  20. #14
    Join Date
    Feb 2009
    Location
    Central CA
    Posts
    401
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by John T View Post
    It's a fancy "third hand"
    I have a gadget that looks like it that holds a dial gauge. Magnetic base--pretty handy...

    Tim

  21. #15
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Don’t you hate it when the garbage men leave the lid open on the can…. I know I do so, did something about it.








    Sent from my iPhone using Tapatalk

  22. Likes hddnis, whtbaron, Weldalittle liked this post
  23. #16
    Join Date
    Nov 2010
    Posts
    130
    Post Thanks / Like

    Re: Crawler007's random welding projects

    that severed arm extra hand would make a good toolbox warning sign against those that "borrow" your tools and "forget" to bring them back. Jim

  24. #17
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,051
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by Lis2323 View Post
    Extremely nice!


    Better than mine …




    Sent from my iPad using Tapatalk
    Did that guy work with oxygen tanks?
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  25. Likes Lis2323, psacustomcreations liked this post
  26. #18
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    looks like a bandsaw accident, to clean to be a cutoff wheel...

  27. Likes whtbaron liked this post
  28. #19
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,051
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Is the spring on your lid light enough to allow the garbage to fall out when they dump them over the truck? How automated is your pickup system? The one thing more annoying than open lids might be garbage cans that don't get emptied.
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  29. Likes SweetMK liked this post
  30. #20
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    They don't use the type of truck that garbs the can and lifts it above the truck and dumps it, if we did Im sure this spring would be light enough to work with that too. Our guys just flip the lid open and pull the bags out and toss them into the truck. They will still be able to do the job they will just have to hold the lid with one hand and reach into the can with the other to grab the bags (I tried it out, its no problem) I didnt want to make there life any harder than it needs to be. I just dont want a trash can thats full of trash smelling water, leaves and racoons.

  31. Likes whtbaron liked this post
  32. #21
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,326
    Post Thanks / Like

    Re: Crawler007's random welding projects

    I think our garbage guys are all working from home atm…..


    Sent from my iPad using Tapatalk
    :

  33. #22
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Well,my boy bought a new to him 07 KX250 and wouldn’t you know it when he got it home the crankcase had a big crack…..

    So we disassembled it


    And split the case to get to the crack just below the crank.


    Took a carbide bit to the cracks and edges inside and out



    Welded it up inside and out, used 4043 filler and it seemed to work pretty good.



    And cleaned up the inside


    Never welded a case before, hopefully it hold up…


    Sent from my iPhone using Tapatalk

  34. Likes N2 Welding, Lis2323, arcflash liked this post
  35. #23
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,079
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Quote Originally Posted by Crawler007 View Post
    Well,my boy bought a new to him 07 KX250 and wouldn’t you know it when he got it home the crankcase had a big crack…..

    So we disassembled it

    And split the case to get to the crack just below the crank.

    Took a carbide bit to the cracks and edges inside and out
    Welded it up inside and out, used 4043 filler and it seemed to work pretty good.

    And cleaned up the inside

    Never welded a case before, hopefully it hold up…
    Nicely done
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  36. #24
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    My dads getting older but he still likes to go out kayak fishing with me. Our kayaks loaded up are quite heavy and some of the launches here in WV are really steep and it’s hard to load the kayaks up at the bottom of the steep ramp. So I added a latch system to his bed extender, it’s not finished I still need to build a pivot so it can swing right and left and lock in the strait on position for hauling.

    Name:  IMG_5878.jpg
Views: 232
Size:  113.8 KB
    Name:  IMG_5877.jpg
Views: 231
Size:  105.9 KB
    I’ll get more pics once I get the materials I need to make the pivot.


    Sent from my iPhone using Tapatalk

  37. Likes whtbaron liked this post
  38. #25
    Join Date
    Nov 2021
    Location
    WV
    Posts
    13
    Post Thanks / Like

    Re: Crawler007's random welding projects

    Name:  IMG_5871.jpg
Views: 232
Size:  175.8 KB
    I added everything painted in red


    Sent from my iPhone using Tapatalk

  39. Likes whtbaron, psacustomcreations liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,108,469.78500 seconds with 13 queries