    Hey there,
    I was contracted to do some welding. They want a time estimate. Can anyone here help me decide how long this should take? I've never done this type of work.
    Its security for a parkade. They need 26 x 8'x4' sheets of expanded steel welded. and 26 smaller pieces at 48"x30".
    I'm using a MIG welder. I feel like I could weld a full size sheet, tack each little point, in less than an hour. Does this sound right?
    Thanks for the help!!

  2. #2
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    1,923
    Post Thanks / Like

    Re: Welding Expanded Steel

    If you think you can do it in an hour give it 1.5 anyway. It isnt welded over paint etc? Test a small one? Did you look at this, dont want to find out its got epoxy paint etc.

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,146
    Post Thanks / Like

    Re: Welding Expanded Steel

    What are welding expanded steel to?
    What Guage is the expanded steel ?
    Do have to weld ever web of the expanded steel or can you skip weld?

    Dave

    Quote Originally Posted by shasdakota View Post
    Hey there,
    I was contracted to do some welding. They want a time estimate. Can anyone here help me decide how long this should take? I've never done this type of work.
    Its security for a parkade. They need 26 x 8'x4' sheets of expanded steel welded. and 26 smaller pieces at 48"x30".
    I'm using a MIG welder. I feel like I could weld a full size sheet, tack each little point, in less than an hour. Does this sound right?
    Thanks for the help!!
    Last edited by smithdoor; 12-02-2021 at 07:16 PM.

  4. #4
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,516
    Post Thanks / Like

    Re: Welding Expanded Steel

    Pics and the thickness and size of the openings would get you more help on this. It would probably be easier to use some 14 ga X 2" flat bar as a backer and weld the expanded to it. IMO it will be quite a challenge to weld the ends together even with a mig using gas shield. I'm trying to visualize why the 48"x30" pieces have to be joined to the 4x8s. Like I said some pics will help.
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  5. #5
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,146
    Post Thanks / Like

    Re: Welding Expanded Steel

    I would buy the expanded steel full size.
    It would give better looking job.

    If I design the job I would use to 2 sizes anger irons for a sandwich. It give a finish look.

    Dave

    Quote Originally Posted by mla2ofus View Post
    Pics and the thickness and size of the openings would get you more help on this. It would probably be easier to use some 14 ga X 2" flat bar as a backer and weld the expanded to it. IMO it will be quite a challenge to weld the ends together even with a mig using gas shield. I'm trying to visualize why the 48"x30" pieces have to be joined to the 4x8s. Like I said some pics will help.

  6. #6
    Join Date
    May 2011
    Posts
    548
    Post Thanks / Like

    Re: Welding Expanded Steel

    If you are welding flat expanded metal, and welding the 30" to the end of a 96" sheet then that would be very simple as they have flat spots on the ends which make good welding tabs. If your welding raised, well that will probably suck. They dont go well together unless it was cut to do that by an experienced cutter.

    Also, expanded metal doesnt come 4x8 it comes like 49.5" x 98 or even 99".

    Sent from my SM-G960U using Tapatalk

  7. #7
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,549
    Post Thanks / Like

    Re: Welding Expanded Steel

    Can you weld? You may be asking the wrong querstons? I would say 1.5 hrs, also. Good luck

  8. #8
    Join Date
    Nov 2010
    Location
    Mid-East
    Posts
    2,620
    Post Thanks / Like

    Re: Welding Expanded Steel

    Quote Originally Posted by shasdakota View Post
    Hey there,
    I was contracted to do some welding. They want a time estimate. Can anyone here help me decide how long this should take? I've never done this type of work.
    Its security for a parkade. They need 26 x 8'x4' sheets of expanded steel welded. and 26 smaller pieces at 48"x30".
    I'm using a MIG welder. I feel like I could weld a full size sheet, tack each little point, in less than an hour. Does this sound right?
    Thanks for the help!!
    Welded to what? Frames? Each other? Why are you welding every point? Is it galvanized?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,643,131,189.83032 seconds with 13 queries