    Tig tungsten diameter: relation to welding current and to metal thickness

    Hi,

    Does anyone have information to how the thickness (diameter) of the (dc) tig-tungsten electrode relates to:
    1. the welding current (amps)
    2. the thickness of the metal to be welded.

    The metal in my focus is plain sheet steel, not galvanised, as used in older cars (guess about 1,2 mm/1.6 mm/2.0 mm).

    Thanks,
    oldwelderman

  2. #2
    Join Date
    Sep 2015
    Location
    West coast of Florida
    Posts
    528
    Post Thanks / Like

    Re: Tig tungsten diameter: relation to welding current and to metal thickness

    For any given tungsten diameter there is a max amps that can be successfully used

    For a given material thickness there is a range of amps that will successfully weld it, depending on material (part) configuration

    Name:  tungsten chart.jpg
Views: 142
Size:  71.2 KB
    Richard
    West coast of Florida

  3. Likes shovelon, leightrepairs liked this post
  4. #3
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,063
    Post Thanks / Like

    Re: Tig tungsten diameter: relation to welding current and to metal thickness

    1/16 and 3/32.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,870,123.88697 seconds with 15 queries