    Tig tungsten diameter: relation to welding current and to metal thickness

    Hi,

    Does anyone have information to how the thickness (diameter) of the (dc) tig-tungsten electrode relates to:
    1. the welding current (amps)
    2. the thickness of the metal to be welded.

    The metal in my focus is plain sheet steel, not galvanised, as used in older cars (guess about 1,2 mm/1.6 mm/2.0 mm).

    Thanks,
    oldwelderman

  2. #2
    Join Date
    Sep 2015
    Location
    West coast of Florida
    Posts
    867
    Post Thanks / Like

    Re: Tig tungsten diameter: relation to welding current and to metal thickness

    For any given tungsten diameter there is a max amps that can be successfully used

    For a given material thickness there is a range of amps that will successfully weld it, depending on material (part) configuration

    Name:  tungsten chart.jpg
Views: 283
Size:  71.2 KB
    Richard
    West coast of Florida
    Website

  3. Likes shovelon, leightrepairs liked this post
  4. #3
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Tig tungsten diameter: relation to welding current and to metal thickness

    1/16 and 3/32.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,280,943.21622 seconds with 20 queries