    OK, the gift wrapping, and unwrapping is over,, and I ate too much,, AND the weather is beautiful this week!!
    I figure it is time to start a project,,

    I haven't done much with the plasma cutter I bought this past summer,, so this project will be plasma cutter intensive,,
    The oil tank I was given is an indoor tank, that was used outdoors,, so, the bottom of the tank resembles a screen door.
    That does not hurt the project,,

    The plus side of the bottom being rusted away,, there is nothing combustible inside of the tank!!
    That all drained, or evaporated a decade ago,,

    So,, what is your guess as to what I am going to try to make out of this 275 gallon fuel oil tank ??

    Hint as to what it is,, I have never seen one this large before, and I watch a LOT of YouTube videos!!

    To start, an end was "precisely plasma cut" maybe, I should say, "plasma cut,, good enough"



    Make your guess,,, please,,

  2. #2
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    The plasma took me a while to get good at. I've self tought myself to move as fast as you can before it kicks back and that's what ruins the tips. I do it by ear a lot too it has a certain sound when its at it's fine line of too fast go much faster and it will kick back. Really fine line between to slow and too fast. Being light handed it the key

  3. Likes SweetMK liked this post
  4. #3
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    That tank was tough to cut, because there is SO MUCH RUST,,

    After I finished cutting, "and the next step", there was over a gallon of rust that had fallen off the inside of the tank.

  5. #4
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,294
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    A steel drum, each spline a different tone.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 140

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  6. Likes SweetMK liked this post
  7. #5
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Bang, BANG, BANG,, the drum is getting some sheetmetal adjustment ??


  8. Likes whtbaron liked this post
  9. #6
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,622
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    You may look a using a guide, wood is ok, also they make stand-offs for the tip of the torch to help keep the cutting distance the same.
    DIY CNC Plasma table USB BOB Price THC
    Hypertherm 65
    Everlast PowerTig 255 EXT
    Miler 180 Mig
    13" metal lathe
    Mill/ Drill
    ECT, ECT,

  10. Likes SweetMK liked this post
  11. #7
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,897
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Burn barrow/ tub.

  12. Likes SweetMK liked this post
  13. #8
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,972
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    I used a 500 gal round tank to aid in a data collection monitor on a small dam site once... wish I'd kept pics now. I didn't have a plasma in those days and I was afraid to take after an ex fuel tank with a torch, so I did the cutting with a zip disc. Went well.
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  14. Likes SweetMK liked this post
  15. #9
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Everyone keeps telling me that I am always trying to put square plugs, in round holes,,
    well, in this case, I took a square (rectangular) tank, and made it into a round shape..


    Boy, won't they be surprised!





    This is why you MUST have at least TWO tractors!!


    Plasma cutter time for the OTHER end,,,





    It appears that two of the cuts went past the mark,, OH NOOOOOOOOOOOO!!!!!!!!!!

  16. Likes whtbaron liked this post
  17. #10
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,972
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    The built in legs are different... all the ones I've seen sat on cradles...
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  18. Likes SweetMK liked this post
  19. #11
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,414
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Rocket Stove ?
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  20. Likes SweetMK liked this post
  21. #12
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Quote Originally Posted by albrightree View Post
    Rocket Stove ?
    That is close, some times, I expect it to sound like a rocket stove,,
    When I started, the tank side was 43" tall, and 27" wide.
    After releasing the chains, there was some spring back, but, the dimensions ended up at 40" high, and 33" wide. That 33" is good enough.



    These tabs are bent in to form a heat shield, reflecting the heat hack in, rather than directly getting to the drum.

    In the very back, you can see the amount of rust that has fallen off the tank, and was trapped in the tank. I think it ended up filling half of a 5 gallon bucket.

    My other option was to cut the end out, and throw it away, this way, the end still serves a purpose,, helping to retain heat.

    The oil drum looked so "Majestic" I figured it needed a "CROWN"!!


  22. #13
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    OK, Part "B" of this project started out as a 55 gallon barrel, with one end removed.
    The barrel was sitting outside, filled with water. As the barrel froze, the ice expanded, and "domed" the closed end.



    I cut a hole in the dome that is the size of a 5 gallon bucket lid.

    Notice the color of the barrel is light rust color, and some yellow.

  23. #14
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Here is a pic of the oil tank, with the Part"B" 55 gallon drum on top,



    It is now ready to burn the half dozen LARGE stumps I have in one field.
    These are big stumps, the trees were over 30" at 5 feet high,
    The stumps are 50 to 60 inches across at ground level.

    This is a fun way to get rid of stumps in the winter, and it gets rid of EVERY bit of brush, and branches that falls off of my other trees.
    Yard cleanup, and some exercise, at the same time! Win-WIN! WOOT!!

  24. #15
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    I filled the oil tank with brush, and branches, logs up to 6 inches in diameter,
    It took WAY more than I expected, I had to make a second trip to the brush pile for more wood.

    A quart of old motor oil was added, a HF propane "Weed Burner" was aimed under the oil tank,
    the fire was blazing in about 3 minutes,,



    Flames are shooting out of the hole in the 55 gallon drum dome, at least 3 feet high.

    This stump burner has been burning over 8 hours today, I went back and added more wood one time.
    I had a ladder next to a trailer, to be able to get high enough to drop wood into the top of the barrel.
    The top of the barrel is right at 8 feet high, I get pretty good draft,, the draft sucks in air at the bottom, incinerating the stump.

  25. Likes Lis2323, whtbaron, albrightree, N2 Welding liked this post
  26. #16
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,414
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Super-sized Chimnea !

    Neighbors might think its a still.https://www.weldingweb.com/images/smilies/drinkup.gif
    Last edited by albrightree; 12-27-2021 at 11:31 PM.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  27. Likes SweetMK liked this post
  28. #17
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Quote Originally Posted by albrightree View Post
    Super-sized Chimnea !

    Neighbors might think its a still.
    THAT would be funny, or possibly just fit in,, I am close to Franklin County, compared to the rest of the members here,,

  29. #18
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Quote Originally Posted by albrightree View Post
    Super-sized Chimnea !

    I wanted to make it 60 feet high, but my wife said NO! to me buying that many barrels!!

  30. #19
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    2,474
    Post Thanks / Like

    Re: Plasma Cutter Project,, WhAtSyOuRgUeSs ??

    Here is another attempt at getting a pic of the flames,,


  31. Likes whtbaron, N2 Welding liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,242,830.54190 seconds with 21 queries