Ahp 201 AC balance
Hi,
I am getting around to tig some aluminum. The orange user manual for my AHP leaves a lot to be desired.
Is the AC Balance knob a percentage of negative to positive in which case, on this machine, i dial to 75% for negative with a 25% cleaning cycle?
The way they word cleaning is a little ambiguous for a newbie.
Thanks
-
-
-
Re: Ahp 201 AC balance
different manufacturers pick different interpretations for the percentage.
To find out empirically, set the cleaning percent to 95%.
If there is very little oxide cleaned area (the white surface next to the weld) then your welder shows the percentage of the time for negative current .
If cleaned area is large and your tungsten wants to melt off, then your welder shows the percentage of time for positive current.
Now adjust to your liking.
MillerMatic 252, HTP 221 w/cooler, Hypertherm PM45, Lincoln IdealArc 250 AC/DC, victor Oxy/Acet
"I'd like to believe as many true things and as few false things as possible"
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Ahp 201 AC balance
Originally Posted by
frieed
different manufacturers pick different interpretations for the percentage.
To find out empirically, set the cleaning percent to 95%.
If there is very little oxide cleaned area (the white surface next to the weld) then your welder shows the percentage of the time for negative current .
If cleaned area is large and your tungsten wants to melt off, then your welder shows the percentage of time for positive current.
Now adjust to your liking.
Thanks. I can do this but I was looking for someone who owns this machine and can just say, then I will just label the knob...I have seen videos where the wrong setting with excess cleaning can produce extreme excitement...I do not want to shatter a cup.
Hey man, Thanks for responding!
-
Re: Ahp 201 AC balance
Jody does a video on the AlphaTIG 200X and covered the settings pretty well. I doubt AHP changed how they mark balance as they came out with minor variations on the machine. He starts with the AC balance at 35% and makes a point to mention that it's 35% electrode positive or 35% cleaning. It's worth watching.
Check out my bench vise website:
http://mivise.com
Miller Syncrowave 250DX
Millermatic 350P with XR AlumaPro
Miller Regency 200 with 22A feeder and Spoolmatic 3
Hobart Champion Elite
Everlast PowerTig 210EXT
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Ahp 201 AC balance
very big thanks. can’t wait to get back home and watch. love this forum!
-
Re: Ahp 201 AC balance
i really just want to label the knob so i will remember next time. i am new to aluminum. love this machine @240v for steel. the pulse settings work for me.
-
Re: Ahp 201 AC balance
ELECTRODE POSITIVE A/C Balance knob for AHP-201