    I have the 350 ext what would be the maximum size rod I could use? I believe that it will not put out 350 amps in Stick mode correct?
    thanks

  2. #2
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    8,961
    Post Thanks / Like

    Re: air arc gouging

    I would like to see this.

  3. #3
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: air arc gouging

    Correct. IIRC the stick output is 270A. It is not made to air arc gouge. It will blow up the unit. It is not designed for this type of long arc, high voltage output. It will also void the warranty. So please do not do this if you have one already. You will need the PowerMTS 400 since it is designed for this operation.
    Last edited by lugweld; 02-12-2022 at 11:25 AM.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,294,502.87595 seconds with 18 queries