    The output of this welder when running is only 50 volts at the 110 AC outlets. I only get a small spark at the stinger. The DC power at the slip rings is 31 Volts. The output from the stater excitation winding is only about 18 Volts measured between leads 4 and 5 at the full wave rectifier diode. I would appreciate any help on what to look for from here.

  2. #2
    Join Date
    Nov 2021
    Posts
    4
    Post Thanks / Like

    Re: Lincoln Weldenpower 225 Code 9010

    If anyone knows what the correct output is for the exciter winding and for the slip rings I would greatly appreciate that information.

  3. #3
    Join Date
    Dec 2014
    Location
    Wasilla, Alaska
    Posts
    198
    Post Thanks / Like

    Re: Lincoln Weldenpower 225 Code 9010

    Lincoln customer service is very helpful, and duaneb55 and ccawc are helpful on this site.

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,624
    Post Thanks / Like

    Re: Lincoln Weldenpower 225 Code 9010

    I don't have the specific values you're looking for but voltage across leads #4 and #5 is AC if you weren't already aware.

    With an almost doubled voltage thru the bridge rectifier makes me suspect it may possibly have one or more failed diodes and giving you false readings. Have you disconnected it and tested for such?
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  5. #5
    Join Date
    Jun 2022
    Posts
    4
    Post Thanks / Like

    Re: Lincoln Weldenpower 225 Code 9010

    I own a machine just like the one you have and had a problem that sounds much like yours. The problem was one of the positive diodes had failed. I replaced both positive diodes and the problem was solved. Iím just a welder and not a mechanic, but I hope this helps.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,665,089,159.97510 seconds with 11 queries