Results 1 to 8 of 8

Thread: 7018 pic

  1. #1
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,220
    Post Thanks / Like

    7018 pic

    Old weld I came across. Whoops, working out new phone.

  2. #2
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    239
    Post Thanks / Like

    Re: 7018 pic

    TPIUWOP, this post is useless with out pictures.
    We've done so much, for so long, with so little. Were now qualified to do anything with nothing !

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,305
    Post Thanks / Like

    Re: 7018 pic

    Like the white snow ❄ photo.

    The old phone worked better

    Dave

    Quote Originally Posted by Sberry View Post
    Old weld I came across. Whoops, working out new phone.

  4. #4
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,220
    Post Thanks / Like

    Re: 7018 pic

    I am working om a new phone, its got its issues.
    Attached Images Attached Images  

  5. Likes whtbaron liked this post
  6. #5
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,305
    Post Thanks / Like

    Re: 7018 pic

    The old weld looks good.
    What is the question?

    Looks like you got phone working too.

    Dave

    Quote Originally Posted by Sberry View Post
    I am working om a new phone, its got its issues.

  7. #6
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    239
    Post Thanks / Like

    Re: 7018 pic

    Im not a welding inspector but those welds will pass.
    We've done so much, for so long, with so little. Were now qualified to do anything with nothing !

  8. #7
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,305
    Post Thanks / Like

    Re: 7018 pic

    About the only inspection is visible. The only time bring out the xray if some fails.
    This way the can hang the contractor and certified welder even after retirement.

    Dave

    Quote Originally Posted by welding1 View Post
    Im not a welding inspector but those welds will pass.

  9. #8
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    7,051
    Post Thanks / Like

    Re: 7018 pic

    Quote Originally Posted by Sberry View Post
    I am working om a new phone, its got its issues.
    Nice work.
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,111,472.93706 seconds with 13 queries