    Added a spool gun to power mig 200 and tested both guns feed wire. Didn't have any argon gas so could complete testing. Went back to it a couple of days later and now neither gun will feed. Im new to this any help would be greatly appreciated. Thought it might be a fuse but can't locate any inside welder.

    Jeff

  2. #2
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Added spool gun to welder tested fine now neither will feed

    Check the control voltage it should be around 24 volts.

    Dave

    Quote Originally Posted by JeffreyIII View Post
    Added a spool gun to power mig 200 and tested both guns feed wire. Didn't have any argon gas so could complete testing. Went back to it a couple of days later and now neither gun will feed. Im new to this any help would be greatly appreciated. Thought it might be a fuse but can't locate any inside welder.

    Jeff

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,243,717.79525 seconds with 20 queries