    Next Job

    Gotta replace a few worn out valves 2x5" and 1x3"

  2. #2
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    Don't know why pic didn't load.

  3. Likes ttoks liked this post
  4. #3
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    You'd expect this to be square coming from chermany. Now I gotta offset the prep to make it square. The 5" valves are smaller in dimensions than the originals so I have to weld in 35mm pups so they can replace like for like.

  5. Likes albrightree, whtbaron, ttoks liked this post
  6. #4
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    One down

  7. #5
    Join Date
    Jan 2022
    Location
    Sugarland, GA
    Posts
    396
    Post Thanks / Like

    Re: Next Job

    Nicely done
    Retired Old Guy

    Hobart 210
    Lincoln AC/DC 225/125
    Evolution 14” Saw

  8. #6
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    Here's the 5" valves I'm to replace

  9. Likes ttoks liked this post
  10. #7
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,357
    Post Thanks / Like

    Re: Next Job

    Looks great 👍.

    Happy for you they want the valves replaced 🙂.

    Dave

    Quote Originally Posted by Woznme View Post
    Here's the 5" valves I'm to replace

  11. #8
    Join Date
    Nov 2021
    Posts
    5
    Post Thanks / Like

    Re: Next Job

    Quote Originally Posted by Woznme View Post
    You'd expect this to be square coming from chermany. Now I gotta offset the prep to make it square. The 5" valves are smaller in dimensions than the originals so I have to weld in 35mm pups so they can replace like for like using it
    Hi, nicely done! What equipment do you use?
    All the best!

  12. #9
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    Thanks!
    I used my Dynasty 200DX as per usual.

    I have a Unimig Razor 200 dc power source as back up but I've never used it. I bought it in a moment of weakness, it's light and easy to get up high roofs, but I'm too one eyed blue.

  13. Likes Bill09, welding1 liked this post
  14. #10
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,357
    Post Thanks / Like

    Re: Next Job

    Your Dynasty 200DX looks like a great great welder. I have had a lot of Miller's in my life and going brand no break downs.

    Dave

    Quote Originally Posted by Woznme View Post
    Thanks!
    I used my Dynasty 200DX as per usual.

    I have a Unimig Razor 200 dc power source as back up but I've never used it. I bought it in a moment of weakness, it's light and easy to get up high roofs, but I'm too one eyed blue.

  15. Likes Bill09 liked this post
  16. #11
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    People complain about the price of Miller. I have buddies who spend 2-3K on their power sources that fail after 3-4years, repairs, replacement, aggrevation, rinse and repeat.
    I've had mine for 10 years now and no probs. Been with me on jobs from one end of the country to the other. That makes mine cheap, right? And it pulses and does ac. I think it's love.

  17. Likes Bill09 liked this post
  18. #12
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    243
    Post Thanks / Like

    Re: Next Job

    I have a Miller DX 200, thing is bad A$$. Many times I'll have it maxed out TIG welding thick Aluminum, to the point I cant hold the torch. It just keeps on running, bought back in 2004 when they were cheap. LOL
    We've done so much, for so long, with so little. Were now qualified to do anything with nothing !

  19. #13
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    The production and weather gods finally lined up and I was able to get in and get the job done including the 3" valve at the far end of the receiver.
    Name:  V3.jpg
Views: 176
Size:  619.1 KB
    Name:  V2.jpg
Views: 177
Size:  372.8 KB


    I was told this is my best side. The pleasure, of course, is all yours!
    Name:  V1.jpg
Views: 176
Size:  627.8 KB

  20. Likes Lis2323, 52 Ford liked this post
  21. #14
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,062
    Post Thanks / Like

    Re: Next Job

    Quote Originally Posted by Woznme View Post
    Name:  V1.jpg
Views: 176
Size:  627.8 KB
    Is this guy alright? Should we call emergency services?
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  22. #15
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,354
    Post Thanks / Like

    Re: Next Job

    Quote Originally Posted by shovelon View Post
    Is this guy alright? Should we call emergency services?
    Woznme catching 40 winks after a rough night.....


    Sent from my iPhone using Tapatalk
    :

  23. Likes 52 Ford liked this post
  24. #16
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    Quote Originally Posted by shovelon View Post
    Is this guy alright? Should we call emergency services?
    Definitely something seriously wrong. For a start he's got a face like a dropped pie. And probably drinks too much

    Name:  Dropped Pie.jpg
Views: 128
Size:  69.5 KB

  25. #17
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,357
    Post Thanks / Like

    Re: Next Job

    Looks like great pie 🥧 😋 👌.
    Did you use the 5 second rule or just let the trash 🗑 can eat that great pie 🥧.
    Next use a metal pan We work metal for a reason you drop metal and it keeps on.

    Dave

    Quote Originally Posted by Woznme View Post
    Definitely something seriously wrong. For a start he's got a face like a dropped pie. And probably drinks too much

    Name:  Dropped Pie.jpg
Views: 128
Size:  69.5 KB

  26. #18
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    505
    Post Thanks / Like

    Re: Next Job

    I get to talk about my good looks, you don't.
    Now I'm offended.
    Pie face matters!! I'm beautiful!!

  27. Likes Lis2323 liked this post
  28. #19
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,354
    Post Thanks / Like

    Re: Next Job

    Quote Originally Posted by Woznme View Post
    I get to talk about my good looks, you don't.
    Now I'm offended.
    Pie face matters!! I'm beautiful!!
    of course. We all know what an inclusive group weldors are…


    Sent from my iPad using Tapatalk
    :

  29. #20
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,357
    Post Thanks / Like

    Re: Next Job

    That pie 🥧 😍
    Your avatar looks great maybe 40.

    Dave

    Quote Originally Posted by Woznme View Post
    I get to talk about my good looks, you don't.
    Now I'm offended.
    Pie face matters!! I'm beautiful!!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,519,335.49377 seconds with 15 queries