    I'm looking to build a motorcycle frame in chromoly.It will be a trellis frame, something like this:



    that's just a quick photoshop to give a rough idea.

    I've built frames in 1018 before, but not in chromoly.

    Is there anything special to know/do when welding chromoly as opposed to mild steel?

    What would be best choice for filler rod? Is argon sufficient or will I need a different gas/mix? Will I need to heat treat the frame after welding to relive welding stresses?

    It will be tacked with MIG and finish welded with TIG.

    Any links or references that may help me out?

    Or should I just stick to 1018 that I have more experience with?

    Cheers.
    Last edited by gr8twhite; 05-15-2022 at 07:43 PM.

  2. #2
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,764
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    I bought a bunch of various filler a while back and 4130 was labeled chrom- moly

    I think it needs post heat treatment???
    I could be wrong

    Ive used it for mild steel welding and it held up fine.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    6,304
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    They use in aircraft a lot of chromoly tubing and welding with torch.
    The only tubing I use is EMT and that I brazing the mid steel tubing.

    Dave

    Quote Originally Posted by gr8twhite View Post
    I'm looking to build a motorcycle frame in chromoly.It will be a trellis frame, something like this:



    that's just a quick photoshop to give a rough idea.

    I've built frames in 1018 before, but not in chromoly.

    Is there anything special to know/do when welding chromoly as opposed to mild steel?

    What would be best choice for filler rod? Is argon sufficient or will I need a different gas/mix? Will I need to heat treat the frame after welding to relive welding stresses?

    It will be tacked with MIG and finish welded with TIG.

    Any links or references that may help me out?

    Or should I just stick to 1018 that I have more experience with?

    Cheers.

  4. Dislikes Louie1961 disliked this post
  5. #4
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,305
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?




    1st on WeldingWeb to have a scrolling sig!



  6. #5
    Join Date
    Oct 2014
    Posts
    1,455
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    Quote Originally Posted by John T View Post
    I bought a bunch of various filler a while back and 4130 was labeled chrom- moly

    I think it needs post heat treatment???
    I could be wrong

    I've used it for mild steel welding and it held up fine.
    Labelled chrome moly because that is what it is not necessarily what you should weld with it.

    4130 rod not needed to weld chrome moly.

    Regular ER70S-2 is the filler used for welding 4130.

    Does not need stress relieving unless thicker than 1/8"

    Good read,

    https://www.millerwelds.com/resource...e-applications
    Last edited by danielplace; 05-16-2022 at 02:11 PM.

  7. Likes John T, Louie1961 liked this post
  8. #6
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,059
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    I think Er80 is the better match for 4130 non hardened weldments. In fact the only filler AWS will offer a SWPS for 4130 is Er80S-B2. But ER80s-D2 is more common and easy to use. ER70 was recommended for non heat treated weldments until Er80 was formulated. Basically they added some 4130 to the Er70 to achieve a better match without a great deal of base metal dilution. If you are going to heat treat your weldment then you must use 4130 filler.

    Only advise though is make sure you have a good cup size and lengthy post flow and when terminating the arc keep the rod and puddle in the gas stream. Otherwise the weld and rod end will contaminate and bubble up horribly upon restart. Then is is hard to get rid of the foaming without grinding out the puddle or using stainless. And if you do think you fried the rod end clip it off. You will find out eventually but beware.

    Actually 4130 is a joy to weld. Clean and the puddle is not watery. The filler is nice and stiff and goes where you put it.

    If your wall thickness is 1/8" or less no prehieat or stress relief is required. More than that preheat and post weld stress relief is recommended.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  9. Likes Louie1961, LtBadd, Jack Ryan liked this post
  10. #7
    Join Date
    Jan 2022
    Location
    Sugarland, GA
    Posts
    384
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    Enjoyed the videos. Thank y’all for this thread
    Retired Old Guy

    Hobart 210
    Lincoln AC/DC 225/125
    Evolution 14 Saw

  11. #8
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,220
    Post Thanks / Like

    Re: anything to know about welding chromoly tube?

    Its probably a fact there is a lot to know about it, how much it all matters I bet has a lot of opinion, Seen a lot of dirt bike stuff welded up fugly with 6011 that actually worked as long as the factory stuff. OA too. Wire feed even better.

  12. Likes XMilitary liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,110,701.85465 seconds with 14 queries