    Help-0, thermistor isn't shorted. XMT 304

    I'm getting an occasional help-0 error (and no "thunk") when I switch this thing on. The service book says it's the thermistor RT2. I've checked the thermistor for proper resistance, and swapped it for a different one and still occasionally have the same issue. Usually I can turn if off and back on once or twice and then it'll turn on and work normally until the next time I try to use it. Any ideas or further troubleshooting I should do for the thermistor?

    Name:  PXL_20220614_020808109.jpg
Views: 100
Size:  173.0 KB
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  2. #2
    Join Date
    Sep 2020
    Location
    VT
    Posts
    312
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    Looking again today I noticed some of the lugs are partially pulled out of the board.

    L1-1 and L1-2. Gonna fix these and see if it makes a difference

    Name:  PXL_20220615_160230035.jpg
Views: 79
Size:  162.8 KB

    Name:  PXL_20220615_160238305.jpg
Views: 77
Size:  152.8 KB
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  3. #3
    Join Date
    Sep 2020
    Location
    VT
    Posts
    312
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    Fixed those lugs, still gave help 0 message at first power on, but then was fine the next couple times. Haven't had another chance to try it since

    Name:  PXL_20220615_182534002.jpg
Views: 64
Size:  119.9 KB

    Name:  PXL_20220615_173156480.MP.jpg
Views: 63
Size:  78.3 KB
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  4. #4
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,348
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    Once it fires up,,, leave it on,, ha

  5. #5
    Join Date
    Sep 2020
    Location
    VT
    Posts
    312
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    That's an idea, could leave the leads connected to discourage unwanted visitors to my shop too
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  6. #6
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,508
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    What's the discoloration at the lead terminal circled in red?
    Attached Images Attached Images  
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  7. #7
    Join Date
    Sep 2020
    Location
    VT
    Posts
    312
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    Dust and grime
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  8. #8
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,508
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    OK. I thought it looked like a bad crimp that has been arcing.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  9. #9
    Join Date
    Sep 2020
    Location
    VT
    Posts
    312
    Post Thanks / Like

    Re: Help-0, thermistor isn't shorted. XMT 304

    New clue: I noticed that whenever it decides to give the Help-0 code, it doesn't make the normal "thunk" noise. So I took the cover off and wiggled the connectors that go to the contactors. Tried again and one contactor "thunked" but the other didn't, and still had Help-0. So I took off all the connectors on the top circuit board and made sure they had a tight electrical connection. Tried it a few times since then and 100% working so far. Now for some serious testing!
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,657,004,818.22389 seconds with 13 queries