    Miller 251 not getting gas

    I have a 04 Miller 251 thatís not getting gas past 20 cfh. Before 20cfh the solenoid works. But past 20cfh it quits. Iíve replaced ( solenoid, liner, regulator) Iíve checked all the hoses. Until I tested the wires that run to the solenoid. There getting 16.4v Iím lost as to what my next steps should be. Do I get a new circuit board?

  2. #2
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,143
    Post Thanks / Like

    Re: Miller 251 not getting gas

    It could the solenoid or the PC board.
    Need to check out solenoid to see if working

    Dave

    Quote Originally Posted by Exsrvs15 View Post
    I have a 04 Miller 251 thatís not getting gas past 20 cfh. Before 20cfh the solenoid works. But past 20cfh it quits. Iíve replaced ( solenoid, liner, regulator) Iíve checked all the hoses. Until I tested the wires that run to the solenoid. There getting 16.4v Iím lost as to what my next steps should be. Do I get a new circuit board?

  3. #3
    Join Date
    Jun 2022
    Posts
    3
    Post Thanks / Like

    Re: Miller 251 not getting gas

    The solenoid does work but only up till 20 CFH

  4. #4
    Join Date
    Jun 2022
    Posts
    3
    Post Thanks / Like

    Re: Miller 251 not getting gas

    I did check the voltage to the solenoid itís not getting 34 V itís getting 16.4. When I checked the two wires that go to the solenoid without the solenoid connected and those are only getting 16 V or so would that mean I need a new PC board

  5. #5
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,540
    Post Thanks / Like

    Re: Miller 251 not getting gas

    I suggest a call to Miller Customer Service in the morning and see if they can walk you through troubleshooting the unit.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,659,933,230.56969 seconds with 13 queries