    Picked up this used cabinet. The rear near the top has been dented in a bit. I took a couple of pics with flat bar so you can see how the rear at the top is pushed in, which caused top near the rear to bulge up.







    Plan is to add casters, put on a plywood top and make this a drill press stand for a 80lb drill press.

    I saw this video from sixtyfiveford where he welds a bolt to the dent and pulls the dent out. Link to video:


    I guess that's the best bet? If there's an easier method, I'm all ears.