    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    3,566
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Arctan
    When you cut the 3/8" stock did you have it standing up in edge or laying flat?
    Material like that needs to be stood up on edge so you are only cutting 3/8 at a time.
    Laying flat is terrible for the blade.

    Sent from my SM-G996U using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  2. #52
    Join Date
    Sep 2020
    Location
    VT
    Posts
    349
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Lesson learned. I had it flat. I need to go back to fabricating preschool
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  3. #53
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,734
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    You can change your display name from your email to something else.

    Contact the Moderator.

    On a different site I do that at less once a week.

    It is easy for the Moderator to do.

    Dave

    Quote Originally Posted by ngoodman@gmail.com View Post
    What is wrong with my metal chop saw?
    When I try to make a cut, my blade is starting to wander instead of holding firm where it is. Does this just mean the blade is dull? Or is there something worse going on?

  4. #54
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,734
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Try Harbor Freight a new 4x6 bandsaw it will over 7½" flat bar and pipe 7½" by rotating half way though the cut too.

    It will last a life time.

    Dave

    Quote Originally Posted by ArcTan View Post
    Anyone have a used bandsaw for sale?

  5. #55
    Join Date
    Sep 2020
    Location
    VT
    Posts
    349
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    So this brings up another question: are these style chop saws only designed for relatively thin material? Sometimes I need to cut things that's would be dimensionally possible to cut, such as a piece of 2" round bar, or a piece of 1-1/4 x 4" steel. I assume trying that would be a bad idea?
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  6. #56
    Join Date
    Sep 2020
    Location
    VT
    Posts
    349
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Quote Originally Posted by smithdoor View Post
    Try Harbor Freight a new 4x6 bandsaw it will over 7½" flat bar and pipe 7½" by rotating half way though the cut too.

    It will last a life time.

    Dave
    Dave, I appreciate the tip. But you seem to be quite optimistic about the quality of tools from Harbor Garbage. Either that or you are pessimistic about how long my lifetime will be.
    I would probably die before I got out of the store if the experience I've had with their tools determined my lifetime!
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  7. Likes whtbaron liked this post
  8. #57
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,974
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    The HF bandsaw will last. However, debatable if it will still be HF tool after one finishing modifying it.

  9. #58
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,734
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    I purchased mind in 2007 works great .
    I have done nothing to saw other than saw blades.

    Dave

    Quote Originally Posted by ArcTan View Post
    Dave, I appreciate the tip. But you seem to be quite optimistic about the quality of tools from Harbor Garbage. Either that or you are pessimistic about how long my lifetime will be.
    I would probably die before I got out of the store if the experience I've had with their tools determined my lifetime!

  10. #59
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,734
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    It only tool from Harbor Freight the have that has no modifications.

    Dave

    Quote Originally Posted by tapwelder View Post
    The HF bandsaw will last. However, debatable if it will still be HF tool after one finishing modifying it.

  11. #60
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,684
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Quote Originally Posted by tapwelder View Post
    The HF bandsaw will last. However, debatable if it will still be HF tool after one finishing modifying it.
    I have the hf larger bandsaw, I buy grizzly parts for it online, it's great,

    Sent from my SM-G973U using Tapatalk

  12. #61
    Join Date
    Jun 2008
    Location
    Central California
    Posts
    4,472
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Quote Originally Posted by ArcTan View Post
    So this brings up another question: are these style chop saws only designed for relatively thin material? Sometimes I need to cut things that's would be dimensionally possible to cut, such as a piece of 2" round bar, or a piece of 1-1/4 x 4" steel. I assume trying that would be a bad idea?
    As with any grinding operation, a number of variables are involved. A fine grain wheel gives a smoother surface but, having more cutting grains in contact, requires more pressure and causes more heating. If cutting thin sections, the pressure per area is reasonable but for wider pieces, the wheel tends to load up and cut poorly unless very hard material is being cut. Using a very coarse-grained wheel improves the situation, as does rotating the work to change the angle-of-approach and lessen the area of contact, usually possible with round, square or angle iron.

    All tools have operations they excel at and others they work poorly for. Normal bandsaws don't do well cutting very hard material and can have trouble with angle cuts, if not set up/watched carefully.
    BTW, some abrasive saws are made with a cam action that constantly changes the cutting head position and thereby changes the area of contact on the work.

  13. Likes ArcTan liked this post
  14. #62
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,734
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    When had shop I added a 4x6 go other saws I had. It would move around shop for cutting small parts.
    The welder or machine could working and saw could cutting parts they needed.

    Dave

    Quote Originally Posted by MetalMan23 View Post
    I have the hf larger bandsaw, I buy grizzly parts for it online, it's great,

    Sent from my SM-G973U using Tapatalk

  15. #63
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,895
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    [QUOTE=smithdoor;8879853]I purchased mind in 2007 works great .
    I have done nothing to saw other than saw blades.

    My HF 4x6 is over 12 years old. Back then it was only $115.00 with a 30% off coupon, yes 30% ! I replaced motor 6 years ago with a used Craftsman motor from a table saw. I buy blades from Farm and fleet , USA made for $12.00 now. I still use it for my small stuff even though I upgraded to an ELLIS 1600. The ELLIS is an amazing saw.

  16. #64
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,642
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Quote Originally Posted by ArcTan View Post
    So this brings up another question: are these style chop saws only designed for relatively thin material? Sometimes I need to cut things that's would be dimensionally possible to cut, such as a piece of 2" round bar, or a piece of 1-1/4 x 4" steel. I assume trying that would be a bad idea?
    You already answered yourself for that situation....

    Quote Originally Posted by ArcTan View Post
    Took almost 8 minutes.
    Quote Originally Posted by ArcTan View Post
    Lesson learned. I had it flat. I need to go back to fabricating preschool
    Your solid 2" round bar or 1¼" x 4" steel would present a very similar situation as to when you had the ⅜" x 2½" laying flat. There is a lot more material to cut at once, thus lengthening the process because the motor is bogging down.
    1st on WeldingWeb to have a scrolling sig!



  17. #65
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    3,566
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    Arctan,
    Make yourself a set of V blocks so you can cut square stock on a diagonal. This presents the lowest profile to the blade and makes it easier on the saw. It wont help on the really thick material, but will also help hold round stock better.

    Name:  V block.jpg
Views: 54
Size:  86.7 KB
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  18. Likes ArcTan, Lis2323 liked this post
  19. #66
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    8,363
    Post Thanks / Like

    Re: What is wrong with my metal chop saw?

    I took advantage of psa’s tip after he posted the idea a few years back….






    Sent from my iPad using Tapatalk
    :

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,048,989.75580 seconds with 15 queries