I have been running a Bernard duraflux gun for fluxcore wire, but it’s for 1/16-3/32 wire, with a fixed liner. I would like to run .035 and .045 fluxcore. What’s a good gun to use? I was thinking a profax 1260.
I have been running a Bernard duraflux gun for fluxcore wire, but it’s for 1/16-3/32 wire, with a fixed liner. I would like to run .035 and .045 fluxcore. What’s a good gun to use? I was thinking a profax 1260.
I was thinking of trying the .035 wire with one of my 400 mig guns. One has a threaded neck, so I’d use a nozzle to protect it. The other slides on, so I may try it without the nozzle.
I found a profax 1260 at a very good price so I’m going that route. I’m still going to try the .035 through my mig gun to see how good it works though.
Has anyone ever tried running .034 or .045 through a duraflux gun with a 1/16-3/32 liner? I can get the tips, and already have the rollers. Is it worth trying?
I finally had some time to try the .035 fluxcore through one of my profax 400 mig guns. It works really well, so I think I’m going to roll with that. Now, I just need to order some .045, and I’ll be set. Thanks for all the input.
Related Threads
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
?
WeldingWeb - Welding Community for pros and enthusiasts
posts
1.8M
members
82K
Since
2003
Community Forum for Welding Professionals and Enthusiasts To Interact and Learn - Free