STAY THE HELL AWAY FROM IT FOR CLEANING METAL OF ANY KIND BEFORE WELDING!!!!!!!!!:nono::nono::nono::nono::nono::nono:
This stuff will KILL YOU.
Read this..
http://www.popsci.com/diy/article/2009-12/dont-get-careless
Ok now got it?
Added..
No brake cleaner/carb cleaner or anything else with chlorine or chlorinated solvents for that matter.