I have a 5000 pound rated open car trailer. The coupler no longer closes and need to replace the a frame. Does anyone have experience with this?
I am going to cut old one off with angle grinder then grind smooth. I have a miller 140. Do u think this is strong enough to weld this on? I have no checked the thickness yet of the a frame. If not I'm going to put a few good tacks with the 140 just to trailer it to friends shop down the block with no weight on it to weld it up with the big welder.
Thanks
I am going to cut old one off with angle grinder then grind smooth. I have a miller 140. Do u think this is strong enough to weld this on? I have no checked the thickness yet of the a frame. If not I'm going to put a few good tacks with the 140 just to trailer it to friends shop down the block with no weight on it to weld it up with the big welder.